A kind of easily colored knitted fabric and production method thereof
A technology for knitted fabrics and production methods, applied in the field of knitted fabrics, can solve the problems of the great difference in dyeing properties of polyester and cotton components, long process flow of two-bath method, complicated dyeing process flow, etc., and achieve concise process steps and reduce hydrolysis. The effect of simple reaction and process flow
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] An easy-to-color knitted fabric, the knitted fabric includes the following raw materials by mass percentage: 45% of natural cotton fibers, 30% of modified polyester fibers, and 25% of blended yarns.
[0032] In this embodiment, the blended yarn is prepared by blending viscose fiber and UHMWPE fiber at a blending ratio of 50%:50% by weight.
[0033] In this embodiment, the preparation method of the modified polyester fiber includes the following steps: adding the polyester fiber to 1 g / L of JFC penetrant, then adding 8 g / L sodium hydroxide solution, and the bath ratio is 1:10, Raise the temperature to 100°C for 60min, drain the waste liquid, add water to wash for 10min, raise the temperature to 60°C, add 1g / L polyester oligomer detergent to wash for 20min, wash with water for 10min, then dehydrate and dry. The modified polyester fiber.
[0034] A production method of the above-mentioned easily colored knitted fabric, comprising the steps:
[0035] A. Blended yarn proce...
Embodiment 2
[0050] An easy-to-color knitted fabric, the knitted fabric comprises the following raw materials by mass percentage: 50% of natural cotton fibers, 35% of modified polyester fibers, and 15% of blended yarns.
[0051] In this embodiment, the blended yarn is prepared by blending viscose fiber and UHMWPE fiber at a blending ratio of 65%: 35% by weight.
[0052] In this embodiment, the preparation method of the modified polyester fiber includes the following steps: adding the polyester fiber to 1.1 g / L of JFC penetrant, then adding 10 g / L sodium hydroxide solution, and the bath ratio is 1:11 , raise the temperature to 120℃ for 45min, drain the waste liquid, add water for washing for 15min, increase the temperature to 70℃, add 1.5g / L polyester oligomer detergent for 25min washing, wash with water for 15min, dehydrate and dry The modified polyester fiber is obtained.
[0053] A production method of the above-mentioned easily colored knitted fabric, comprising the steps:
[0054] A....
Embodiment 3
[0069] An easy-to-color knitted fabric, the knitted fabric comprises the following raw materials by mass percentage: 60% of natural cotton fibers, 30% of modified polyester fibers, and 10% of blended yarns.
[0070] In this embodiment, the blended yarn is prepared by blending viscose fiber and UHMWPE fiber at a blending ratio of 70%: 30% by weight.
[0071] In this embodiment, the preparation method of the modified polyester fiber includes the following steps: adding the polyester fiber to 1.2g / L of JFC penetrant, then adding 10g / L sodium hydroxide solution, and the bath ratio is 1:12 , raise the temperature to 130°C for 30min, drain the waste liquid, add water for cleaning for 20min, raise the temperature to 70°C, then add 2g / L polyester oligomer detergent for 30min cleaning, rinse with water for 20min, dehydrate and dry. The modified polyester fiber is obtained.
[0072] A production method of the above-mentioned easily colored knitted fabric, comprising the steps:
[0073...
PUM
Login to View More Abstract
Description
Claims