High-temperature salt deposition resisting agent
A technology of salt formation and high temperature, applied in water pollutants, water/sewage treatment, water/sludge/sewage treatment, etc., can solve global environmental hazards, damage to the ecological environment and human health, lack of treatment and disposal, etc. question
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0012] A high-temperature anti-salt agent, prepared from the following components in parts by weight: the proportioning of ATMP is 25%, the proportioning of HEDP is 20%, the proportioning of EDTMPS is 10%, the proportioning of EDTMPA is 7%, the proportioning of DTMPPA 12%, TH-904 3%, PESA 13% and PASP 10%.
[0013] Material preparation steps: Put ATMP and HEDP into the container according to the ratio and mix them evenly, then put them in the mixer, then add EDTMPS to get the primary mixture. During the mixing process, use a sealed mixer with the outer wall made of glass and the inner mixing rod made of stainless steel. , during the mixing process, run at low speed and prolong the mixing time. Fully mix EDTMPA, DTMPPA and TH-904 to obtain the first mixture, then put EDTMPA, DTMPPA and TH-904 into the container and stir evenly to obtain the second For the mixture, use a glass container for mixing during the mixing process, mix the secondary mixture by stirring during the mixing...
Embodiment 2
[0018] A high-temperature anti-salt agent, prepared from the following components in parts by weight: the proportioning of ATMP is 27%, the proportioning of HEDP is 18%, the proportioning of EDTMPS is 8%, the proportioning of EDTMPA is 6%, the proportioning of DTMPPA 10%, TH-904 3%, PESA 18% and PASP 10%.
[0019] Material preparation steps: Put ATMP and HEDP into the container according to the ratio and mix them evenly, then put them in the mixer, then add EDTMPS to get the primary mixture. During the mixing process, use a sealed mixer with the outer wall made of glass and the inner mixing rod made of stainless steel. , during the mixing process, run at low speed and prolong the mixing time. Fully mix EDTMPA, DTMPPA and TH-904 to obtain the first mixture, then put EDTMPA, DTMPPA and TH-904 into the container and stir evenly to obtain the second For the mixture, use a glass container for mixing during the mixing process, mix the secondary mixture by stirring during the mixing ...
Embodiment 3
[0024] A high-temperature anti-salt agent, prepared from the following components in parts by weight: the proportioning of ATMP is 22%, the proportioning of HEDP is 23%, the proportioning of EDTMPS is 11%, the proportioning of EDTMPA is 6%, the proportioning of DTMPPA 12%, TH-904 4%, PESA 15% and PASP 10%.
[0025] Material preparation steps: Put ATMP and HEDP into the container according to the ratio and mix them evenly, then put them in the mixer, then add EDTMPS to get the primary mixture. During the mixing process, use a sealed mixer with the outer wall made of glass and the inner mixing rod made of stainless steel. , During the mixing process, run at low speed and prolong the mixing time. Fully mix EDTMPA, DTMPPA and TH-904 to obtain the first mixture, then put EDTMPA, DTMPPA and TH-904 into the container and stir evenly to obtain the second For the mixture, use a glass container for mixing during the mixing process, mix the secondary mixture by stirring during the mixing...