Emulified and modified asphalt and its prepn
A technology for emulsifying modified asphalt and emulsifiers, which is applied in the processing of tar asphalt/petroleum asphalt/natural asphalt, and the petroleum industry, and can solve the problems of restricting the popularization and application of slurry seal technology, strong temperature sensitivity, and poor flexibility , to achieve the effect of shortening the closing time of traffic, excellent performance and obvious effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0017] 1. Preparation of modified asphalt
[0018] (1) When the temperature of the base asphalt reaches 150-170°C, add 1-20% (accounting for the weight percentage of the base asphalt) of SBS modifier to fully disperse and swell;
[0019] (2) Pass the swollen matrix asphalt and SBS through a high-speed shear mill to achieve refinement and further dispersion;
[0020] (3) Under the condition of 140-190°C, incubate for a certain period of time to make qualified modified asphalt.
[0021] 2. Preparation of emulsion
[0022] Add quantitative emulsifier, stabilizer, water, hydrochloric acid and other materials into the mixer and mix thoroughly. The temperature is controlled at 60-95° C., and an aqueous emulsion with an emulsifier content of 1-10% is prepared.
[0023] 3. Put the modified asphalt and the emulsion in the ratio of (1-4): 1 at the same time through the emulsification mill, then mechanically stir and defoam to make the emulsified modified asphalt.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More