Embodiment 1
[0012] A method for delaying fouling of the sieve plate of an extraction tower includes:
[0013] (1) Introduce the condensate from the low-pressure steam of the phosphoric acid concentration production system into the heat exchanger, and the temperature of the condensate is about 120°C;
[0014] (2) The extractant to be added to the extraction tower is introduced into the heat exchanger to exchange heat with the condensate entering the heat exchanger to increase the temperature of the extractant; the extractant is controlled by adjusting the amount of condensate entering the heat exchanger Temperature, by adjusting the temperature of the extractant, control the temperature difference between the acid temperature in and out of the tower at 10°C.
[0015] (3) The extractant with elevated temperature is fed into the extraction tower to extract iodine from phosphoric acid.
Embodiment 2
[0017] A method for delaying fouling of the sieve plate of an extraction tower includes:
[0018] (1) Introduce the condensate from the low-pressure steam of the phosphoric acid concentration production system into the heat exchanger, and the temperature of the condensate is about 120°C;
[0019] (2) The extractant to be added to the extraction tower is introduced into the heat exchanger to exchange heat with the condensate entering the heat exchanger to increase the temperature of the extractant; the extractant is controlled by adjusting the amount of condensate entering the heat exchanger Temperature, by adjusting the temperature of the extractant, control the temperature difference between the acid temperature in and out of the tower at 20°C.
[0020] (3) The extractant with elevated temperature is fed into the extraction tower to extract iodine from phosphoric acid.
Embodiment 3
[0022] A method for delaying fouling of the sieve plate of an extraction tower includes:
[0023] (1) Introduce the condensate from the low-pressure steam of the phosphoric acid concentration production system into the heat exchanger, and the condensate temperature is about 100℃;
[0024] (2) The extractant to be added to the extraction tower is introduced into the heat exchanger to exchange heat with the condensate entering the heat exchanger to increase the temperature of the extractant; the extractant is controlled by adjusting the amount of condensate entering the heat exchanger Temperature, by adjusting the temperature of the extractant, control the temperature difference between the acid temperature in and out of the tower at 5°C.
[0025] (3) The extractant with elevated temperature is fed into the extraction tower to extract iodine from phosphoric acid.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com