Pearl yarn and method for producing same
A production method and yarn technology, applied in the field of pearlescent yarn preparation, can solve the problems of unfavorable health and environmental protection, not washable, not durable, etc., and achieve the effect of ensuring strength, soft luster and rich colors
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for producing pearlescent yarn with 32s / 1 long-staple cotton+80s / 1 long-staple cotton, comprising the following processing steps:
[0026] 1. Spinning
[0027] Spin high-quality long-staple cotton into 32s / 1 and 80s / 1 yarns respectively;
[0028] The twist of 32s / 1 thick yarn is spun according to the minimum equipment, the twist is 62 twists / 10CM, and the twist coefficient is 265;
[0029] The 80s / 1 fine yarn is spun according to the conventional knitting yarn twist, the twist is 130 twists / 10CM, and the twist coefficient is 350.
[0030] 2. Joint stock merger
[0031] According to the characteristics of the two-for-one twisting machine, a thin yarn is wrapped and coiled around a thick yarn. The twist is 53 twists / 10CM, and the twist coefficient is 272.
Embodiment 2
[0033] A method for producing colored cotton yarn with pearl luster by 40s / 1 dyed yarn+80s / 1 compact spinning, comprising the following processing steps:
[0034] 1. Spinning
[0035] Spin high-quality long-staple cotton into 40s / 1 and 80s / 1 yarns respectively;
[0036] The twist of 40s / 1 thick yarn is spun according to the minimum equipment, the twist is 53 twists / 10CM, and the twist coefficient is controlled at 272;
[0037] The 80s / 1 fine yarn is spun according to the normal twist of the knitting yarn, the twist is 130 twists / 10CM, and the twist coefficient is 350.
[0038] 2. Single yarn dyeing
[0039] Dye 40s / 1 into colored yarn.
[0040] 3. Joint stock merger
[0041] According to the characteristics of the two-for-one twister, the thinner yarn is wrapped and wrapped around the thicker yarn, the twist is 58 twists / 10CM, and the twist coefficient is controlled at 272.
Embodiment 3
[0043] A kind of method with 40s / 1 hemp cotton (90 / 10)+80s / 1 silk cotton (75 / 25) produces the colored cotton yarn with pearl luster, comprises following processing steps:
[0044] 1. Spinning
[0045] Select high-quality linen cotton to be spun into linen cotton 90 / 10 40s / 1 yarn, and high-quality silk cotton to be spun into 75 / 25 80s / 1 yarn;
[0046] 40s / 1 yarn spinning technical parameters of hemp cotton 90 / 10, the twist is 53 twists / 10CM, and the twist coefficient is controlled at 272;
[0047] 80s / 1 yarn spinning technical parameters of silk cotton 75 / 25, the twist is 130 twists / 10CM, and the twist coefficient is 350.
[0048] 2. Single yarn dyeing
[0049] Dye 40s / 1 of hemp cotton 90 / 10 and 80s / 1 of silk cotton 75 / 25 in different colors.
[0050] 3. Joint stock merger
[0051] According to the characteristics of the two-for-one twisting machine, the thinner yarn is wrapped and wound around the thicker yarn. The twist is 58 twists / 10CM, and the twist coefficient is 272...
PUM
| Property | Measurement | Unit |
|---|---|---|
| twist factor | aaaaa | aaaaa |
| twist factor | aaaaa | aaaaa |