A production method and rigidity-enhancing technology, which is applied in the field of automotive interior parts production, can solve problems such as deformation, complex components of coat racks, and insufficient rigidity, and achieve the effects of ensuring accuracy, improving operating efficiency, and reducing weight
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Produce Mitsubishi Motors 3X45 car coat rack, its specification is: 1250×610mm.
[0014] The production method of the rigidity-enhanced automobile coat rack comprises the following steps:
[0015] a. Put the base material of the car coat rack into the oven for heating between the upper oven heating plate and the lower oven heating plate. When heating, the temperature of the upper oven heating plate is controlled at 280~290°C, and the temperature of the lower oven heating plate is controlled at 330°C ~340℃, the heating time is controlled at 150~170 seconds;
[0016] b. Put the heated car coat rack base material into the forming punching machine, and bury the prefabricated car coat rack base material in the surface of the lower mold of the forming punching machine and in the middle position corresponding to the left and right sides of the center line of the car coat rack Rigidity enhanced deck, rigidity enhanced deck with vertical corners;
[0017] c. Start the molding ...
Embodiment 2
[0021] Produce General Motors E11 car coat rack, its specification is: 1360×780mm.
[0022] The production method of the rigidity-enhanced automobile coat rack comprises the following steps:
[0023] a. Put the base material of the car coat rack into the oven for heating between the upper oven heating plate and the lower oven heating plate. When heating, the temperature of the upper oven heating plate is controlled at 320~340°C, and the temperature of the lower oven heating plate is controlled at 380 ~400℃, the heating time is controlled at 110~120 seconds;
[0024] b. Put the heated car coat rack base material into the forming punching machine, and bury the prefabricated car coat rack base material in the surface of the lower mold of the forming punching machine and in the middle position corresponding to the left and right sides of the center line of the car coat rack Rigidity enhanced deck, rigidity enhanced deck with corners;
[0025] c. Start the molding punching machin...
Embodiment 3
[0029] Produce Shanghai Automobile IS12 car coat rack, its specification is: 1480×1120mm.
[0030] The production method of the rigidity-enhanced automobile coat rack comprises the following steps:
[0031] a. Put the base material of the car coat rack into the oven for heating between the upper oven heating plate and the lower oven heating plate. When heating, the temperature of the upper oven heating plate is controlled at 230~260°C, and the temperature of the lower oven heating plate is controlled at 320°C ~360℃, the heating time is controlled at 340~360 seconds;
[0032] b. Put the heated car coat rack base material into the forming punching machine, and bury the prefabricated car coat rack base material in the surface of the lower mold of the forming punching machine and in the middle position corresponding to the left and right sides of the center line of the car coat rack Rigidity enhanced deck, rigidity enhanced deck with corners;
[0033] c. Start the molding punchi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com