A heating element and heating component technology, which is applied to heating devices, hypodermic injection devices, contraceptives, etc. for treatment and treatment, can solve the problems of peeling, low-temperature scald, discomfort in use, etc., and achieves no discomfort, maintains independence, The effect of relieving the burden on the skin
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1)
[0152] Made of nylon non-woven fabric with a length of 70mm and a width of 75mm (weight per unit area 40g / m 2 ) on a base material composed of a polyethylene layer with a length of 70mm, a width of 75mm, and a thickness of 40μm. 40g / m 2 ) is laminated with a polyethylene porous film with a length of 100 mm, a width of 115 mm, and a thickness of 70 μm. The base material and the coating material are sealed around the periphery of the heat-generating composition to form a heat-generating component. An adhesive composed of an acrylic solvent-based adhesive was applied (coating thickness: 23 μm) to prepare the heating element of Example 1.
Embodiment 2)
[0154] The heat generating element of Example 2 provided a protective sheet with a length of 80 mm, a width of 85 mm, and a thickness of 0.38 mm on the heat generating member of the heat generating element of Example 1.
[0155] For the protective sheet, a polyethylene film with a thickness of 28 μm is laminated on a metallocene polyethylene film with a thickness of 12 μm, and a coating amount of 6±1 g / m is applied on it. 2 Coated with acrylic adhesive, using lamination with a weight per unit area of 55±5g / m 2 100% rayon fiber non-woven fabric structure, the non-woven fabric is placed on the sensor side of the tester and placed on the heat generating part.
[0156] In addition, temperature measurement was carried out under the following measurement conditions.
[0157] [Temperature measurement test of heating part]
[0158] (A) Test conditions
[0159] ?Ambient temperature: 20±1.5℃
[0160] ・Placing table: A heater with a hose joint for circulating hot water with a heigh...
Embodiment 3)
[0170] Next, in order to further verify the effectiveness of the protective sheet, an example in which the basis weight and raw materials of the nonwoven fabric were changed will be described.
[0171] It is made of man-made fiber spunlace non-woven fabric with a length of 70mm and a width of 75mm (the weight per unit area is 45g / m 2 ) is laminated with a polyethylene resin film with a thickness of 40 μm to place the exothermic composition on the substrate, and the exothermic composition is covered with a spunlace nonwoven fabric made of PET with a length of 70 mm and a width of 75 mm (weight per unit area: 30 g / m 2 ) on a covering material formed by laminating a polyethylene resin porous film with a thickness of 70 μm, and sealing the substrate and the covering material around the exothermic composition to form a heat generating member. Moreover, the mesh sheet (weight per unit area: 40 g / m 2 ), apply an adhesive made of acrylic solvent-based adhesive (coating thickness: 23 ...