A natural rock flake paint and white paint technology, applied in the field of decorative paint, can solve the problems of poor weather resistance and water resistance, difficult to master technology, long production cycle, etc., and achieve the effects of good weather resistance, simple production process and short production cycle
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] A preparation method of natural rock flake paint, the steps are:
[0028] 1) Preparation of white paint: first weigh 0.2% of wetting agent, 0.4% of defoamer, 60% of silicon-acrylic emulsion, 3% of film-forming aid, 3% of hydrophobically modified associative thickener, 0.3% of multifunctional auxiliary agent, 0.3% of polyurethane, 0.3% of bactericidal preservative, and 32.5% of water; Stir at high speed for 30 minutes, then add emulsion and film-forming aids and continue to stir at 500 rpm for 20 minutes until the mixture is uniform, then add hydrophobically modified associative thickener and polyurethane thickener, and finally add antiseptic 2) preparation of finished paint: take 20% of rock flakes and 80% of white paint successively by weight percentage, stir at a low speed for 40 minutes at a speed of 50 rpm, wait until even to get natural rock flake finished paint, and pass the inspection Then pack it.
Embodiment 2
[0030] A preparation method of natural rock flake paint, the steps are:
[0031] 1) Preparation of white paint: first weigh 0.25% of wetting agent, 0.35% of defoamer, 36% of silicon-acrylic emulsion, 5% of film-forming aid, 3% of hydrophobically modified associative thickener, Multifunctional auxiliary agent 0.2%, polyurethane 0.8%, bactericidal preservative 0.2%, water 54.2%; then water, wetting agent, defoamer, multifunctional auxiliary agent are added in the agitator successively, with 300 rpm / hour Stir at high speed for 40 minutes, then add emulsion and film-forming aids and continue to stir at 300 rpm for 25 minutes until the mixture is uniform, then add hydrophobically modified associative thickener and polyurethane thickener, and finally add sterilizing 2) preparation of finished paint: take 35% of rock flakes and 65% of white paint successively by weight percentage, stir at a low speed for 30 minutes at a speed of 80 rpm, wait until even to get the finished paint of na...
Embodiment 3
[0033] A preparation method of natural rock flake paint, the steps are:
[0034] 1) Preparation of white paint: first weigh 0.35% of wetting agent, 0.25% of defoamer, 60% of silicon-acrylic emulsion, 3.4% of film-forming aid, 1.5% of hydrophobically modified associative thickener, Multifunctional auxiliary agent 0.4%, polyurethane 0.5%, bactericidal preservative 0.1%, water 31.5%; then water, wetting agent, defoamer, multifunctional auxiliary agent are added to the mixer in sequence, and the Stir at high speed for 20 minutes, then add emulsion and film-forming aids and continue to stir at 800 rpm for 10 minutes until the mixture is uniform, then add hydrophobically modified associative thickener and polyurethane thickener, and finally add sterilizing 2) Preparation of finished paint: take 30% of rock flakes and 70% of white paint successively by weight percentage, stir at a low speed for 60 minutes at a speed of 50 rpm, wait until even to get natural rock flake finished paint,...