Bushing mold for drain pipe of bridge deck and method for applying bushing mold
A technology for drainage pipes and bushings, which is applied in bridges, bridge parts, bridge construction, etc., can solve the problems of poor economical efficiency of drainage pipes, labor and materials, pollution of bridge deck and bottom plate, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0227] Example 1 (The diameter of the discharge pipe is 200 mm, the inner diameter of the lower part of the discharge pipe is 114mm, the wall thickness is 7mm, the thickness of the bridge deck is 50cm, and the bottom of the discharge pipe extends 2cm from the bottom of the bridge deck)
[0228] Specification and size table of mould for bridge deck drain pipe bushing
[0229]
[0230] Note: 1. The length unit is mm;
[0231] 2. The length of the template support rod is the horizontal projection length.
[0232] In the table: "Z"-shaped formwork support rod single length horizontal projection length = discharge pipe pore radius-middle pipe outer wall radius + (20~30mm) = discharge pipe pore radius 200 / 2-middle pipe outer wall radius 24 / 2+30 =118mm, the "Z" formwork support rod is formed by bending a single square steel twice, and the length direction is in a "Z" shape; when the umbrella structure of the bushing mold is fully expanded, the "Z" shape has a horizontal and a bridge The b...
Embodiment 2
[0233] Example 2 (The diameter of the discharge pipe is 220 mm, the outer diameter of the lower part of the discharge pipe is 134mm, the wall thickness is 7mm, the thickness of the bridge deck is 50cm, and the bottom of the discharge pipe does not protrude from the bottom of the bridge deck)
[0234] Specification and size table of mould for bridge deck drain pipe bushing
[0235]
[0236] Note: 1. The unit is mm;
[0237] 2. The length of the template support rod is the horizontal projection length.
example 2
[0238] Example 2 The inner diameter of the drain pipe is larger than that of Example 1, and the bottom of the drain pipe does not protrude from the bottom of the bridge deck. Also, the bushing mold of Example 1 can be used to ensure that the umbrella structure of the bushing mold can penetrate through the hollow part of the drain pipe when the umbrella structure is completely closed. , The height between the upper and lower horizontal top surfaces of the "Z"-shaped formwork support rod, that is, the length of the drain pipe extending from the bottom of the bridge deck, is replaced by a circular plastic foam block.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 