Embodiment 1
[0021] 1. Graphene / Fe 3 o 4 / Preparation of gold nanocomposites
[0022] 1.1 First prepare graphene oxide, the hummers method can be utilized [W. S. Hummers, R. E. Offeman, Preparation of graphitic oxide, Journal of The American Chemical Society 80(1958) 1339-1339.].
[0023] 1.2 For the preparation of gold nanoparticles, refer to the method of Jana [N. R. Jana, L. Gearheart, C. J. Murphy, Wetchemical synthesis of high aspect ratio cylindrical gold nanorods, Journal of Physical Chemistry B 105 (2001) 4065-4067.].
[0024]1.3 Sonicate graphene oxide (1 mg / mL) for 40 minutes, take 7.2 ml into a round bottom flask, then add 30 ml ethylene glycol, 0.054 g FeCl 3 ·6H 2 O, 0.033 g sodium citrate, 0.150 g anhydrous sodium acetate, 0.05 g polyethylene glycol and 10 ml nano-gold, stirred for 30 min, poured into a 50 ml autoclave, and reacted at 200 °C for 10 h. After the reaction is over, the reaction product is washed with ethanol for 3-5 times with the assistance of a magnet.
...
PUM