A kind of yak wool fiber weaving carpet and weaving method
A fiber weaving and yak wool technology is applied in the field of textiles, which can solve the problems of rough carpet textiles and weaving methods that do not use yak wool fibers, and achieve the effect of smooth carpet surface and increased income.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0024] Embodiment 1: A yak wool fiber woven carpet in this embodiment is composed of multiple yak wool yarns, and each yak wool yarn is composed of three yak wool yarns.
specific Embodiment approach 2
[0025] Specific implementation mode two: combination figure 1 with figure 2 Describe this embodiment, the specific steps of a kind of yak fiber weaving carpet weaving method described in this embodiment are as follows:
[0026] Step 1, blending yak velvet fiber thread: select yak velvet with a length of 32 mm and 20% to 30% wild tussah silk to blend into yak velvet fiber thread;
[0027] Step 2, dyeing: dyeing the yak wool fiber thread;
[0028] Step 3. Start weaving the carpet:
[0029] Step 3 (1), Winding: Ply the yarn through the winder and form a ball;
[0030] Step 3 (2), upper warp and tie: use wire hooks to evenly arrange the cotton yarns on the upper and lower beams of the carpet weaving machine beam to form a curtain-like structure, and tie the buckles;
[0031] Step 3 (3), copying the drawing: copy the blue draft drawing on the point drawing through the light-transmitting desktop;
[0032] Step 3 (4), laying the foundation: use cotton yarn to arrange horizontal...
specific Embodiment approach 3
[0041] Specific embodiment three: in the step 2 of a kind of yak fiber woven carpet weaving method described in this embodiment, the specific steps of dyeing yak wool fiber thread are as follows:
[0042] Step A, cleaning: use sodium hypochlorite with a concentration not higher than 8%, and soak for 30 minutes at a water temperature of about 30 degrees Celsius;
[0043] Step B, dyeing: water temperature 80-90 degrees Celsius, put in the corresponding pigment and continue heating for 2 hours;
[0044] Step C, color fixation: use a sulfuric acid solution with a concentration not greater than 5%, and the water temperature is about 30 degrees, for 30 minutes;
[0045] Step D, Rinse: Rinse continuously with clean water for about 10 minutes to remove floating color and sulfuric acid residue;
[0046] Step E. Use a dryer to get rid of the main moisture, and then enter the drying room at about 100 degrees Celsius for 2 hours.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com