Manufacturing method of rinsing-free pearl powder face mask without rinsing
A production method, the technology of pearl powder, applied in the field of beauty and cosmetics, can solve the problems of inconvenient cleaning, easy to flow to the neck hair, discomfort, etc., and achieve the effect of cleaning
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0016] This embodiment is to make a ready-to-use facial mask for 1 person. The raw materials used in this pearl powder disposable facial mask are as follows: 15g of pearl powder, 5g of polyvinyl alcohol powder, 5g of hyaluronic acid, 1g of sodium alginate, 1g of glycerin, poly Oxyethylene sorbitan monooleate 0.5g, camellia oil 0.5g, clove oil 0.45g, sodium lauryl sulfate 0.25g, cinnamon oil 0.05g, distilled water 20g, milk 25g.
[0017] The production method is as follows:
[0018] A. Put the vinyl alcohol powder into the reaction container, add 10g of distilled water at 70-80°C, stir until the polyvinyl alcohol powder is fully dissolved, and obtain a polyvinyl alcohol solution for later use;
[0019] B. Put sodium alginate into a reaction vessel, add 10 g of distilled water at 60-70°C, stir until the sodium alginate is fully dissolved, and obtain a sodium alginate solution for later use;
[0020] C. In a water bath at 70-80°C, mix the polyvinyl alcohol solution obtained in s...
Embodiment 2
[0024] This embodiment is an industrial production of 2000 person-times of facial masks that need to be packaged. The raw materials used for this pearl powder disposable facial mask are as follows: 40kg of pearl powder, 14kg of polyvinyl alcohol powder, 15kg of hyaluronic acid, 5kg of glycerin, 4kg of sodium alginate, poly Oxyethylene sorbitan monooleate 2 kg, camellia oil 1 kg, clove oil 4.5 kg, sodium lauryl sulfate 0.8 kg, cinnamon oil 0.5 kg, distilled water 56 kg, milk 30 kg.
[0025] The production method is as follows:
[0026] A. Put the vinyl alcohol powder into a reaction container, add 10kg of distilled water at 70-80°C, stir until the polyvinyl alcohol powder is fully dissolved, and obtain a polyvinyl alcohol solution for later use;
[0027] B. Put sodium alginate into a reaction vessel, add 10kg of distilled water at 60-70°C, stir until the sodium alginate is fully dissolved, and obtain a sodium alginate solution for later use;
[0028] C. In a water bath at 70-8...