A kind of 3D mobile phone battery cover processing method
A mobile phone battery and processing method technology, applied in the direction of batteries, battery pack components, circuits, etc., can solve problems such as affecting user use, poor wear resistance, reducing battery service life, etc., achieve good economic and social benefits, and increase surface beauty. , the effect of increasing the surface color
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] see figure 1 Shown, a kind of 3D mobile phone battery cover processing method, its method comprises the steps:
[0033] Step A: Cutting: After purchasing large sheets of raw materials, cut them into sheets of reasonable size according to internal needs;
[0034] Step B: UV transfer printing: the sheet cut in step A is transferred into corresponding textures by UV using photocurable glue;
[0035] Step C: First film coating: In step B, the surface of the sheet after UV transfer is covered with a low-viscosity PE film;
[0036] Step D: coating: electroplating an optical film on the sheet after the first film coating in step C;
[0037] Step E: Second coating: cover the surface of the sheet after coating in step D with a layer of low-viscosity PE film;
[0038] Step F: printing ink for the first time: put the ink on the sheet after the second film coating in step E into a baking oven at a certain temperature and bake for a period of time;
[0039] Among them, the bakin...
Embodiment 2
[0053] see figure 1 Shown, a kind of 3D mobile phone battery cover processing method, its method comprises the steps:
[0054] Step A: Cutting: After purchasing large sheets of raw materials, cut them into sheets of reasonable size according to internal needs;
[0055] Step B: UV transfer printing: the sheet cut in step A is transferred into corresponding textures by UV using photocurable glue;
[0056] Step C: First film coating: In step B, the surface of the sheet after UV transfer is covered with a low-viscosity PE film;
[0057] Step D: coating: electroplating an optical film on the sheet after the first film coating in step C;
[0058] Step E: Second coating: cover the surface of the sheet after coating in step D with a layer of low-viscosity PE film;
[0059] Step F: printing ink for the first time: put the ink on the sheet after the second film coating in step E into a baking oven at a certain temperature and bake for a period of time;
[0060] Among them, the bakin...