Graphene electrothermal film health-care mat production method
A production method and graphene technology, applied in phototherapy, radiotherapy, treatment, etc., can solve the problems of electrothermal effect and health care function that cannot meet the demand, and achieve excellent physiotherapy and health care effect, controllable shape, and high safety factor.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Below in conjunction with embodiment the production method of the graphene electric heating film health pad of the present invention is described in further detail.
[0022] First make resin component A: take liquid bisphenol A epoxy resin, 1,4-butanediol diglycidyl ether, and silane coupling agent KH560 with a weight ratio of 60, 4, 1, 0.5, 33, and 1.5, respectively , antifoaming agent BYKA-555, aluminum hydroxide powder, fumed silica, mix evenly; then make resin component B: take liquid polyamide resin with weight ratio of 36, 10, 23, 30, 1 respectively, amino-terminated Liquid nitrile rubber, aluminum hydroxide powder, talcum powder, fumed silica, and mix well;
[0023] Making graphene powder dispersion: take graphene powder, and use dispersion equipment to evenly disperse graphene powder into component A of heat-resistant resin;
[0024] Mixing: mix the resin B component with the dispersion in the above step C and stir evenly;
[0025] Backing board production: Cu...
Embodiment 2
[0031] The difference between this example and Example 1 is that this example makes resin A component: liquid bisphenol A type epoxy resin, 1,4- Butanediol diglycidyl ether, silane coupling agent KH560, defoamer BYKA-555, aluminum hydroxide powder, fumed silica, mix evenly; make resin component B: the weight ratio is 40, 12, 20 respectively , 27.5, 1.5 liquid polyamide resin, amino-terminated liquid nitrile rubber, aluminum hydroxide powder, talcum powder, fumed silica, and then mix well.
Embodiment 3
[0033] The difference between this embodiment and Example 1 is that the resin A component is made: liquid bisphenol A type epoxy resin and 1,4-butanediol with a weight ratio of 60, 5, 3, 0.5, 30, 1.5 respectively Diglycidyl ether, silane coupling agent KH560, defoamer BYKA-555, aluminum hydroxide powder, fumed silica, mix well;
[0034] Make resin component B: take liquid polyamide resin with a weight ratio of 36, 11, 25, 27.9, and 0.1, amino-terminated liquid nitrile rubber, aluminum hydroxide powder, talcum powder, and fumed silica, and mix them evenly. In the embodiment, the target language is set to 20, and the set time value is set to 2.5 seconds.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com