Detergent compositions containing salts of polyetheramines and polymeric acid
A composition and detergent technology, applied in the direction of detergent composition, coating detergent composition, surface active detergent composition, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0143] Under the trade name Baxxodur 2.5 g polyetheramine(2-aminomethylethyl)-omega-(2-aminomethylethoxy)-poly(oxo(methyl-1,2-ethanediyl) sold by (BASF) ) were added to 10.0 g of an aqueous solution of a 50% by weight copolymer of acrylic acid and maleic acid at room temperature. The copolymer of acrylic acid and maleic acid has an average molecular weight Mn of about 70,000 g / mol (measured by gel permeation chromatography, calibrated with polystyrene sulfonic acid) and a molar ratio of acrylic acid to maleic acid of 4:1. The temperature was increased to 50°C. The mixture was stirred for an additional 1 h without external heating. Water was removed in vacuo (0.7 mbar). After trituration, 4.5 g of white, odorless crystals are obtained. pH of a 10% solution in water: 6.
Embodiment 2
[0145] Under the trade name Baxxodur 25.0 g of polyetheramine(2-aminomethylethyl)-omega-(2-aminomethylethoxy)-poly(oxo(methyl-1,2-ethanediyl) sold by (BASF) ) were added to 100.0 g of a 50% by weight aqueous solution of acrylic acid homopolymer in sodium salt at room temperature. The sodium salt of the homopolymer of acrylic acid has a molecular weight of about 4,000 g / mol (measured by gel permeation chromatography, calibrated with polystyrenesulfonic acid). The temperature was raised to 41 °C. The mixture was stirred for an additional 2 hours at 60°C. Water was removed in vacuo (0.7 mbar). After grinding, 70.0 g of pale yellow crystals were obtained. A 10% solution in water has a pH of 6.
Embodiment 3
[0147] 62.5 g of polyether derived from 2-butyl-2-ethyl-1,3-propanediol, alkoxylated with 2.0 mol of propylene oxide per OH, and aminated (amine value 278.2 mg KOH / g) The amine was added to 250.0 g of an aqueous solution of a 50% by weight copolymer of acrylic acid and maleic acid at room temperature. The copolymer of acrylic acid and maleic acid has a molecular weight of about 70,000 g / mol (measured by gel permeation chromatography, calibrated with polystyrene sulfonic acid) and a molar ratio of acrylic acid to maleic acid of 4:1. The temperature was increased to 50 °C. The mixture was stirred at 60 °C for an additional 2 hours. Water was removed in vacuo (0.7 mbar). After grinding, 85.0 g of white, odorless crystals are obtained. A 10% solution in water has a pH of 6, water content: 0.9%.
PUM
| Property | Measurement | Unit |
|---|---|---|
| Bursting strength | aaaaa | aaaaa |
| Boiling point | aaaaa | aaaaa |
| Average molecular weight | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com