Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Softening treatment method for salix integra

A softening treatment and willow technology, applied in wood treatment, wood treatment details, reed/straw treatment, etc., can solve problems such as unsatisfactory effects and environmental hazards, and achieve the effect of improving softening quality and efficiency, and the overall method is simple

Inactive Publication Date: 2017-10-17
FUNAN TENGBO ARTS & CRAFTS CO LTD
View PDF4 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, boiling and steam fumigation are mostly used for the softening treatment of wicker. Although the processing technology is simple, the effect of softening treatment is not ideal. Adding acid, alkali and other ingredients, its softening effect on wicker has been improved, but most of the added substances are harmful to the environment, and the flexibility and other properties of the treated wicker still need to be further improved

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] A softening treatment method of willow barberry, comprising the steps of:

[0025] (1) Treatment of willow bark:

[0026] First, steam and peel the bark willow, then immerse it in the salt solution for 15 minutes, take it out, and finally rinse it with clean water for later use;

[0027] (2) Preparation of softening solution:

[0028] a. Excavate the soil from the peach tree planting field, then mix it with clear water 6 times its total mass, and filter it after high-speed stirring and dispersing for 45 minutes. Concentrate the filtrate to 20% of the original volume to obtain the soil extract for subsequent use;

[0029] b. Mix Phellodendron Phellodendron, Bean Root, Neem Leaf, Bergamot, Honeysuckle, and Houttuynia cordata according to the weight ratio of 15:5:8:3:2:4, then mix with water 5 times its total mass, heat and boil After processing for 1 hour, filter, and concentrate the filtrate to 30% of the original volume to obtain the Chinese medicine extract for subse...

Embodiment 2

[0039] A softening treatment method of willow barberry, comprising the steps of:

[0040] (1) Treatment of willow bark:

[0041] First, steam and peel the willow bark, then immerse it in the salt solution for 18 minutes, take it out, and finally rinse it with water for later use;

[0042] (2) Preparation of softening solution:

[0043] a. Excavate the soil from the peach tree planting field, then mix it with clear water 7 times its total mass, and then filter it after high-speed stirring and dispersion treatment for 47 minutes. After the filtrate is concentrated to 25% of the original volume, the soil extract is obtained for subsequent use;

[0044] b. Mix Phellodendron Phellodendron, Bean Root, Neem Leaf, Bergamot, Honeysuckle, and Houttuynia cordata according to the weight ratio of 16:6:9:4:3:5, then mix with water 6 times its total mass, heat and boil After processing for 1.5h, filter, and concentrate the filtrate to 35% of the original volume to obtain the Chinese medici...

Embodiment 3

[0054] A softening treatment method of willow barberry, comprising the steps of:

[0055] (1) Treatment of willow bark:

[0056] First, steam and peel the willow bark, then immerse it in the salt solution for 20 minutes, take it out, and finally rinse it with clean water for later use;

[0057] (2) Preparation of softening solution:

[0058] a. Excavate the soil from the peach tree planting field, then mix it with clear water 8 times its total mass, and filter it after high-speed stirring and dispersing treatment for 50 minutes. After the filtrate is concentrated to 30% of the original volume, the soil extract is obtained for subsequent use;

[0059] b. Mix Cortex Phellodendri, Bean Root, Neem Leaf, Bergamot, Honeysuckle, and Houttuynia cordata in a weight ratio of 18:7:10:5:4:6, then mix it with water 7 times its total mass, heat and boil After processing for 2 hours, filter, and concentrate the filtrate to 40% of the original volume to obtain the Chinese medicine extract for...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a softening treatment method for salix integra. The method comprises the following steps: (1) treating salix integra; (2) preparing a softening solution; and (3) performing softening treatment. According to the method disclosed by the invention, the salix integra softening treatment process is reasonably improved, the overall method is simple, safe and environmentally friendly, the softening quality and efficiency of the salix integra are effectively improved, and the method is favorable for development of the peach tree planting industry.

Description

technical field [0001] The invention belongs to the technical field of willow weaving processing, and in particular relates to a method for softening willow bark. Background technique [0002] Funan County, affiliated to Fuyang City, Anhui Province, is an early inland development area, located in the northwest of Anhui Province, on the north bank of the junction of the upper and middle reaches of the Huaihe River. Funan County is known as "Famous Specialty Products County" and "Natural Resource Bank". It is a major grain production county in the country, the hometown of willow weaving in China, and the only agricultural (forestry) circular economy demonstration pilot county in the country. Funan is the national willow weaving county. Township, willow products are sold abroad. [0003] Softening treatment is required during the willow weaving process, because the hardness of the naturally harvested wicker is relatively high, and the flexibility cannot meet the requirements f...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): B27K3/50B27K5/06B27K9/00
CPCB27K5/06B27K3/50B27K9/002
Inventor 腾博
Owner FUNAN TENGBO ARTS & CRAFTS CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products