A technology for playgrounds and slides, which is applied in the field of playground slides, can solve problems such as discomfort, poor processing technology, and poor slide materials, and achieve the effects of optimizing the process, increasing interest in playing, and improving the spirit of unity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0028] A preparation process for a playground slide material, comprising the following steps:
[0029] S1. Cleaning and drying, 200 parts of feldspar sandstone, 240 parts of magnetite, 340 parts of chlorite, 250 parts of garnet, 190 parts of quartz stone, 200 parts of talc, shell The mixture A composed of 320 parts and 320 parts of fish bones is placed in a cylindrical container with a through hole, then rinsed with a tap water gun for 30 minutes, and then placed under the fan, the fan speed is set at 1000 rpm, and the time is 5 Minutes to obtain dry mixture A;
[0030] S2. Crushing the ore, put the dry mixture A obtained in S1 into the DF-4 electromagnetic ore pulverizer, drive the vibrating tube to beat the pulverized material at high speed (3000 times / min), and pulverize it into a particle size of 130 mesh mixed powder C;
[0031] S3. Air-dried plants, 320 parts of licorice, 15 parts of bellflower, 410 parts of aloe, 200 parts of Chlorophytum, 250 parts of Sansevieria, 20...
Embodiment 2
[0036] A preparation process for a playground slide, comprising the following steps:
[0037] S1. Cleaning and drying, 230 parts of feldspar sandstone, 280 parts of magnetite, 350 parts of chlorite, 290 parts of garnet, 260 parts of quartz stone, 220 parts of talc, shell The mixture A consisting of 360 parts and 360 parts of fish bones is placed in a cylindrical container with a through hole, then rinsed with a tap water gun for 40 minutes, and then placed under the fan, set the fan speed to 1000 rpm, and the time is 60 Minutes to obtain dry mixture A;
[0038] S2. Crushing the ore, put the dry mixture A obtained in S1 into the DF-4 electromagnetic ore pulverizer, drive the vibrating tube to beat the pulverized material at high speed (3000 times / min), and pulverize it into a particle size of 140 mesh mixed powder C;
[0039] S3. Air-dried plants, consisting of 360 parts of licorice, 20 parts of bellflower, 440 parts of aloe, 230 parts of Chlorophytum, 300 parts of Sansevieri...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com