Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Skin repairing composition and preparation and use method thereof

A technology of skin repair and composition, applied in the field of skin repair composition, can solve the problems such as difficult wound healing and affecting the quality of life, and achieve the effects of shortening time, accelerating repair, and reducing melanin production

Inactive Publication Date: 2018-02-02
苏州汇涵医用科技发展有限公司
View PDF16 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Only a few people's wounds are easy to heal, and most people's wounds are difficult to heal or form severe scars, which seriously affects the quality of life

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] A) Preparation of component A:

[0028] Dissolve 1 g of metallothionein and 0.002 g of recombinant human epidermal growth factor with 400 g of pure water under stirring, then filter, fill and freeze-dry at -20°C for 20 hours to obtain component A;

[0029] B) Preparation of component B:

[0030] a) To prepare the first solution, first dissolve 0.07g of proanthocyanidins, 3g of vitamin C and 0.1g of vitamin E with 190g of pure water under stirring, then add 5g of allantoin and 0.04g of seabuckthorn seed oil and continue stirring until dissolved to obtain the first solution, ready to use;

[0031] b) To prepare the second solution, first dissolve 100 g of sodium pyrrolidone carboxylate and 5 g of copper pyrrolidone carboxylate with stirring with 500 g of pure water, then add 45 g of stearyl alcohol and 80 g of isopropyl myristate and continue stirring until dissolved to obtain The second solution, stand-by;

[0032] c) Prepare the third solution, dissolve 0.1 g of meth...

Embodiment 2

[0036] A) Preparation of component A:

[0037]Dissolve 0.04 g of metallothionein and 0.04 g of recombinant human epidermal growth factor with 420 g of pure water under stirring, then filter, fill and freeze-dry at -20°C for 24 hours to obtain component A;

[0038] B) Preparation of component B:

[0039] a) To prepare the first solution, first dissolve 0.02g of proanthocyanidins, 0.01g of vitamin C and 1.2g of vitamin E with 200g of pure water under stirring, then add 0.02g of allantoin and 0.09g of seabuckthorn seed oil and continue stirring until dissolved, Obtain the first solution, stand-by;

[0040] b) To prepare the second solution, first dissolve 5 g of sodium pyrrolidone carboxylate and 100 g of copper pyrrolidone carboxylate with stirring with 200 g of pure water, then add 60 g of stearyl alcohol and 5 g of isopropyl myristate and continue to stir until dissolved to obtain The second solution, stand-by;

[0041] c) Prepare the third solution, dissolve 1 g of methyl ...

Embodiment 3

[0044] A) Preparation of component A:

[0045] Dissolve 0.08g of metallothionein and 0.008g of recombinant human epidermal growth factor with 500g of pure water under stirring, then filter, fill and freeze-dry at -20°C for 28 hours to obtain component A;

[0046] B) Preparation of component B:

[0047] a) To prepare the first solution, first dissolve 1.5g of proanthocyanidins, 5g of vitamin C and 0.01g of vitamin E with 195g of pure water under stirring, then add 1.2g of allantoin and 1.8g of seabuckthorn seed oil and continue stirring until dissolved to obtain the second One solution, ready to use;

[0048] b) To prepare the second solution, first dissolve 25 g of sodium pyrrolidone carboxylate and 85 g of copper pyrrolidone carboxylate with stirring with 300 g of pure water, then add 85 g of stearyl alcohol and 15 g of isopropyl myristate and continue stirring until dissolved to obtain The second solution, stand-by;

[0049] c) Prepare the third solution, dissolve 5 g of ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention relates to a skin repairing composition and a preparation and use method thereof. The method comprises the steps that 400-500 g of purified water is used for dissolving 0.004-0.2 g of metallothionein and 0.002-0.04 g of recombinant human epidermal growth factors, filtering, filling and free-drying are conducted in sequence, and a component A is obtained; 190-210 g of purified water is used for dissolving 0.02-5 g of procyanidine, 0.01-5 g of vitamin C and 0.01-4 g of vitamin E, 0.02-5 g of allantoin and 0.04-6 g of seabuckthorn seed oil are added, dissolving is conducted, and a first solution is obtained; 200-500 g of purified water is used for dissolving 5-100 g of sodium pyrrolidonecarboxylate and 5-100 g of copper pyrrolidonecarboxylate, 5-100 g of octadecanol and 5-80 g of isopropyl myristate are added, dissolving is conducted, and a second solution is obtained; 190-210 g of purified water is used for dissolving 0.1-5 g of preservative, and a third solution is obtained; the first solution, the second solution and the third solution are mixed to be uniform, filtering and filling are conducted, and a component B is obtained.

Description

technical field [0001] The invention belongs to the technical field of medical surgical medicine and its preparation, in particular relates to a skin repairing composition, and also relates to a preparation method thereof. Background technique [0002] The skin is the largest organ in the human body. It protects various tissues and organs in the body from physical, mechanical, chemical and pathogenic microorganisms. The skin has two barrier functions: one is to prevent the loss of water, electrolytes, and other substances in the body; the other is to prevent the invasion of harmful substances from the outside. The skin maintains the stability of the internal environment of the human body, and the skin also participates in the metabolic process of the human body. [0003] With the development of society, various wound problems appear more and more frequently. According to statistics, about 1% of the world's population is plagued by persistent wound problems, and about 5% o...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Applications(China)
IPC IPC(8): A61K38/18A61P17/00A61P17/02A61P17/18A61K36/185A61K31/4166A61K31/4015A61K31/352A61K31/375A61K31/355A61K38/16
CPCA61K9/0014A61K31/352A61K31/355A61K31/375A61K31/4015A61K31/4166A61K36/185A61K38/16A61K38/1808A61K2300/00
Inventor 徐祥华秦建新冯永良
Owner 苏州汇涵医用科技发展有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products