A simple soft-pack four-electrode lithium-ion battery test system
A lithium-ion battery and four-electrode technology, which is applied in the field of simple soft-pack four-electrode lithium-ion battery test system, can solve the problems of blocking lithium ion migration channels, low success rate, harsh environmental requirements, etc., to increase statistical significance , Potential control is precise, and the effect of increasing reliability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026] Both the annular positive electrode sheet 4 and the square positive electrode sheet 3 are made of lithium iron phosphate material, the annular negative electrode sheet 1 and the square negative electrode sheet 2 are both made of graphite material, and the formulas of the annular positive electrode sheet 4 and the square positive electrode sheet 3 include active materials, conductive agents and bonding agents. agent, the formula of ring-shaped positive electrode sheet 4 and square positive electrode sheet 3 includes active material, conductive agent and binding agent, the proportion of active material is 80% ~ 98%, the proportion of conductive agent is 1% ~ 10%, the proportion of binding agent The ratio is 1%~10%, and the coating surface density of the pole piece is 15mg / cm 2 ~40mg / cm 2 , the formulation of ring-shaped negative electrode sheet 1 and square negative electrode sheet 2 contains active material, conductive agent and binding agent, the formulation of ring-sha...
Embodiment 2
[0032]The annular positive electrode sheet 4 is made of lithium iron phosphate material, and the annular negative electrode sheet 1 is made of graphite material. The formulation of the ring-shaped positive electrode sheet 4 includes an active material, a conductive agent, and a binder. The formulations of the ring-shaped positive electrode sheet 4 and the square positive electrode sheet 3 include an active material, a conductive agent, and a binder, and the proportion of the active material is 80% to 98%. , the proportion of conductive agent is 1%~10%, the proportion of binder is 1%~10%, and the coating surface density of pole piece is 15mg / cm 2 ~40mg / cm 2 . The formula of annular negative electrode sheet 1 includes active material, conductive agent, and binding agent, the formula of annular positive electrode sheet 4 and square positive electrode sheet 3 includes active material, conductive agent and binding agent, and the proportion of active material is 80% ~ 98% , the pr...