Feed acidifying agent and preparation method thereof

A technology of feed acidifier and hydrochloric acid, which is applied in the direction of animal feed, application, and additional food elements, etc., can solve problems such as difficult production processes, reduce the chance of infection, and improve the effect of enzyme activity in the digestive tract

Inactive Publication Date: 2018-05-11
珠海天凯生物科技有限公司
View PDF5 Cites 4 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, there is no report on the use of hydrochloric acid in conjunction with commonly used organic acids. The main...

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Feed acidifying agent and preparation method thereof
  • Feed acidifying agent and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0024] A feed acidifier, comprising the following raw materials:

[0025] Hydrochloric acid 2g, citric acid 10g, lactic acid 8.0g, fumaric acid 10g, malic acid 9.0g, bentonite 20g, starch 30g and acrylic resin 11g.

[0026] Preparation:

[0027] Include the following steps:

[0028] 1) firstly add hydrochloric acid and bentonite into the mixer and mix evenly, the mixing time is 15 minutes;

[0029] 2) Then add citric acid, lactic acid, fumaric acid, malic acid and starch into the mixer, and mix evenly for 10 minutes to obtain soft material;

[0030] 3) Put the soft material prepared in step 2) in a rocking machine, and shake it with a 30-mesh screen to make granules;

[0031] 4) Dry the granules obtained in step 3) in a fluidized bed at 60°C, and pass through a 40-mesh sieve after drying;

[0032] 5) Make a coating solution from acrylic resin, put the granules in a coating pan, and coat them with the coating solution. After spraying the coating solution, dry it in the coat...

Embodiment 2

[0034] A feed acidifier, comprising the following raw materials:

[0035] Hydrochloric acid 5.5g, citric acid 6.0g, acetic acid 12.5g, fumaric acid 9.5g, malic acid 4.0g, bentonite 27.0g, silicon dioxide 28g and carnauba wax 7.5g.

[0036] Preparation:

[0037] Include the following steps:

[0038] 1) firstly add hydrochloric acid and bentonite into the mixer and mix evenly, the mixing time is 17 minutes;

[0039] 2) Then add citric acid, lactic acid, fumaric acid, malic acid and silicon dioxide into the mixer, and mix evenly for 8 minutes to obtain a soft material;

[0040] 3) Put the soft material prepared in step 2) in a rocking machine, and shake it with a 30-mesh screen to make granules;

[0041] 4) Dry the granules obtained in step 3) in a fluidized bed at 60°C, and pass through a 60-mesh sieve after drying;

[0042] 5) Make a coating liquid from carnauba wax, put the granules in a coating pan, and coat them with the coating liquid. After the coating liquid is spraye...

Embodiment 3

[0044] A feed acidifier, calculated by weight percentage, comprising the following raw materials:

[0045] Hydrochloric acid 10.0g, citric acid 10.0g, formic acid 15.0g, fumaric acid 25.0g, lactic acid 20.0g, bentonite 10.0g, silicon dioxide 5.0g and ethyl cellulose 5.0g.

[0046] Preparation:

[0047] Include the following steps:

[0048] 1) firstly add hydrochloric acid and bentonite into the mixer and mix evenly, the mixing time is 13 minutes;

[0049] 2) Then add citric acid, formic acid, fumaric acid, lactic acid and silicon dioxide into the mixer, and mix evenly for 12 minutes to obtain a soft material;

[0050] 3) Put the soft material prepared in step 2) in a rocking machine, and shake it with a 30-mesh screen to make granules;

[0051] 4) Dry the granules obtained in step 3) in a fluidized bed at 60°C, and pass through a 20-mesh sieve after drying;

[0052] 5) Make ethyl cellulose into a coating solution, put the granules in a coating pan, and coat with the coatin...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a feed acidifying agent and a preparation method thereof. The feed acidifying agent comprises 1-10 wt% of hydrochloric acid, 20-80 wt% of an organic acid, 1-30 wt% of bentonite,5-30 wt% of a filler and 5-30 wt% of a coating material. The preparation method comprises the following steps: 1) adding the hydrochloric acid and bentonite into a mixer, and uniformly mixing the hydrochloric acid with bentonite; 2) adding the organic acid and the filler into the mixer, and uniformly mixing above materials to obtain a soft material; 3) placing the soft material prepared in step 2) in a swing machine, and swinging the soft material by a screen to prepare granules; 4) drying the granules obtained in step 3) in a boiling bed, and allowing the dried granules to go through a screen; and 5) processing the coating material to form a coating solution, placing the granules in a coating pan, coating the granules by using the coating solution, drying the coated granules after spraying of the coating solution is completed, and allowing the dried coated granules to go through the screen in order to obtain the feed acidifying agent. The hydrochloric acid and the organic acid are successfully cooperatively used to make the acidifying agent have a good pH value adjusting effect, and has a stronger inhibition effect on existing acidifying agents.

Description

technical field [0001] The invention belongs to the technical field of acid preparations, and in particular relates to a feed acidifier and a preparation method thereof. Background technique [0002] Feed acidifier is an important additive after antibiotics, alongside probiotics, enzyme preparations, and microecological preparations. It is an environmentally friendly additive with no residue, no drug resistance, and no toxic effects. Feed acidifier, as a new type of additive that can reduce the pH value of feed in the digestive tract and provide the most suitable digestive tract environment for animals, has been widely used at home and abroad. Acidifiers are widely used in the feed of poultry, piglets, beef cattle, dairy cows, sheep and other animals. [0003] Feed acidifiers are mostly used in combination with organic acids and inorganic acids, because the combined use of the two can achieve complementary synergistic effects and overcome the shortcomings and defects of a s...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): A23K20/00A23K50/30
Inventor 张晓明麦耀权朱帆
Owner 珠海天凯生物科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products