A production method and technology for decorative painting, applied in the field of metal enamel, can solve the problems of affecting the coloring of the surface glaze layer, short service life of the inkjet cloth, dangerous replacement operation, etc., achieving easy control of firing temperature, easy control of firing time, Reduce the effect of the flattening process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0030] A method for making a decorative painting on an aluminum plate, comprising the following steps:
[0031] Step 1, select a fresh aluminum plate, and use physical or chemical methods to derust and degrease the surface of the aluminum plate;
[0032] Step 2, preparing a transition glaze layer, the mass ratio of each component of the transition glaze layer is: 20 parts of metal aluminum powder, 30 parts of aluminosilicate mineral powder, 20 parts of low-temperature frit powder, 10 parts of potassium oxide, water 60 copies;
[0033] Step 3, uniformly mix the components described in step 2, stir for 30 minutes, and let stand for 10 minutes;
[0034] Step 4, stand up the aluminum plate vertically, and use a spray gun to spray the transition glaze layer prepared in step 3 onto the treated surface of the aluminum plate;
[0035] Step 5: Use the glass tempering furnace horizontal firing method to preliminarily fire the aluminum plate that has been sprayed with the transition gl...
Embodiment 2
[0046] A method for making a decorative painting on an aluminum plate, comprising the following steps:
[0047] Step 1, select a fresh aluminum plate, and use physical or chemical methods to derust and degrease the surface of the aluminum plate;
[0048]Step 2, preparing a transition glaze layer, the mass ratio of each component of the transition glaze layer is: 25 parts of metal aluminum powder, 40 parts of aluminosilicate mineral powder, 25 parts of low-temperature frit powder, 15 parts of potassium oxide, water 65 copies;
[0049] Step 3, uniformly mix the components described in step 2, stir for 40 minutes, and let stand for 15 minutes;
[0050] Step 4, stand up the aluminum plate vertically, and use a spray gun to spray the transition glaze layer prepared in step 3 onto the treated surface of the aluminum plate;
[0051] Step 5: Use the glass tempering furnace horizontal firing method to preliminarily fire the aluminum plate that has been sprayed with the transition gla...
Embodiment 3
[0062] A method for making a decorative painting on an aluminum plate, comprising the following steps:
[0063] Step 1, select a fresh aluminum plate, and use physical or chemical methods to derust and degrease the surface of the aluminum plate;
[0064] Step 2, preparing a transition glaze layer, the mass ratio of each component of the transition glaze layer is: 30 parts of metal aluminum powder, 60 parts of aluminosilicate mineral powder, 30 parts of low-temperature frit powder, 30 parts of potassium oxide, water 70 copies;
[0065] Step 3, uniformly mix the components described in step 2, stir for 60 minutes, and let stand for 30 minutes;
[0066] Step 4, stand up the aluminum plate vertically, and use a spray gun to spray the transition glaze layer prepared in step 3 onto the treated surface of the aluminum plate;
[0067] Step 5: Use the glass tempering furnace horizontal firing method to preliminarily fire the aluminum plate that has been sprayed with the transition gl...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology