Circular bead machining method
A processing method and ball technology, which is applied in the field of jewelry parts processing, can solve the problems of inability to guarantee the shape, precision and production efficiency of balls, and achieve the effect of avoiding low cutting precision and avoiding waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0056] Prepare a strip-shaped gold plate with a width of 19mm and a thickness of 0.18mm, then anneal the gold plate at about 2000 degrees Celsius and cool it to room temperature, and then let the gold plate pass through the round hole with a diameter of 6.0mm , to form a pipe material; the pipe material is kneaded and then welded, first passing through a round hole with a diameter of 5.5mm in the hole line plate, and then passing through a round hole with a diameter of 5.0mm in the hole line plate to form a round tube. The round tube is cut again to form small sections of about 4.6mm, and then the steps of rounding, annealing, rounding, grinding and pickling are carried out successively to obtain round beads.
Embodiment 2
[0058] Prepare a strip-shaped gold plate with a width of 19mm and a thickness of 0.18mm, then anneal the gold plate at about 2000 degrees Celsius and cool it to room temperature, and then let the gold plate pass through the round hole with a diameter of 6.0mm , to form a pipe material; the pipe material is kneaded and then welded, first passing through a round hole with a diameter of 5.0 mm in the round hole line plate, and then passing through a round hole with a diameter of 5.0 mm in the round hole line plate to form a round tube. The round tube is cut again to form small sections of about 4.6mm, and then the steps of rounding, annealing, rounding, grinding and pickling are carried out successively to obtain round beads.
Embodiment 3
[0060] Prepare a strip-shaped gold plate with a width of 19mm and a thickness of 0.18mm, then anneal the gold plate at about 2000 degrees Celsius and cool it to room temperature, and then let the gold plate pass through the round hole with a diameter of 6.0mm , to form a pipe material; the pipe material is kneaded and then welded, first passing through a round hole with a diameter of 5.5mm in the hole line plate, and then passing through a round hole with a diameter of 5.0mm in the hole line plate to form a round tube. The round tube is cut again to form small sections of about 4.6mm, and then the steps of rounding, pressing round, grinding and pickling are carried out successively to obtain round beads.