A technology of ionic liquid and gold leaching agent, applied in the field of gold leaching agent and gold leaching, can solve the problem that there is not much research on ionic liquid extraction of elemental gold, and achieve the effects of low price, reduced cost and low overall energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0036] 1-butyl-3-methylimidazolium chloride salt, sodium dichloroisocyanurate and water prepare compound ionic liquid according to the amount of substance 1:0.2:30, get 3g 1-butyl-3-methylimidazolium chloride salt , 0.75g of sodium dichloroisocyanurate and 9.3ml of water were mixed evenly at room temperature to obtain 10.8ml of solution, and 0.003g of gold powder was added to continue stirring. The gold powder was completely dissolved in 5 minutes, and the Au concentration of the solution was measured by atomic absorption spectrometer to be 277.8ug / ml , Calculate the rate of melting gold to be 100%.
Embodiment 2
[0038] 1-butyl-3-methylimidazolium chloride salt, sodium dichloroisocyanurate and water prepare compound ionic liquid according to the amount of substance 1:0.2:10, get 3g 1-butyl-3-methylimidazolium chloride salt , 0.75g of sodium dichloroisocyanurate and 3.1ml of water were mixed evenly at room temperature to obtain 4.6ml of solution, and 0.003g of gold powder was added to continue stirring. After 4 minutes, the gold powder was completely dissolved, and the Au concentration of the solution was measured by atomic absorption spectrometer to be 652.2ug / ml , Calculate the rate of melting gold to be 100%.
Embodiment 3
[0040] 1-butyl-3-methylimidazolium chloride salt, sodium dichloroisocyanurate and water prepare compound ionic liquid according to the amount of substance 1:0.1:30, get 3g 1-butyl-3-methylimidazolium chloride salt , 0.38g of sodium dichloroisocyanurate and 9.3ml of water were mixed uniformly at room temperature to obtain 10.8ml of solution, and 0.003g of gold powder was added to continue stirring. The gold powder was completely dissolved in 5 minutes, and the Au concentration of the solution was measured by atomic absorption spectrometer to be 277.1ug / ml , The calculated rate of gold dissolution is 99.8%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com