A technology of allelochemicals and composite materials, which is applied in the fields of botanical equipment and methods, chemical instruments and methods, and applications, can solve the problems such as the inability to achieve sustained and high-efficiency algae-inhibiting effects, and achieve good application prospects, convenient operation, and production technology. simple effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0025] The invention provides a method for preparing an allelochemical slow-release magnetized lightweight composite material, comprising the following steps:
[0026] Calcining and acid leaching the open-pore expanded perlite in sequence to obtain pretreated open-pore expanded perlite;
[0027] Mixing the pretreated open-pore expanded perlite, ferric chloride, ethylene glycol, polyethylene glycol and sodium acetate, and performing magnetization by hydrothermal synthesis to obtain magnetized expanded perlite;
[0028] The magnetized expanded perlite and the allelochemical are blended, impregnated, and then dried to obtain a slow-release magnetized lightweight composite material of the allelochemical, and the allelochemical is lactic acid.
[0029] In the invention, the open-pore expanded perlite is sequentially calcined and acid leached to obtain the pretreated open-pore expanded perlite.
[0030] In the present invention, the expanded perlite is preferably ground into powder...
Embodiment 1
[0048] Weigh 3g of open-cell expanded perlite, put it into a 450°C muffle furnace for calcination for 6h, then put it into a beaker filled with 200mL, 50% concentration of sulfuric acid, and then move the beaker to a 500r / min magnetic stirrer for stirring After stirring for 6 hours, it was washed and filtered with suction, and finally placed in a drying oven at 60°C, and dried for 12 hours to obtain white pretreated open-pore expanded perlite.
[0049] Weigh 1.08g ferric chloride (FeCl 3 ·6H 2 O) Dissolved in 32mL of ethylene glycol to obtain a mixed solution, weighed 0.4g of pretreated open-pore expanded perlite and put it into the mixed solution, stirred for 10min with a magnetic stirrer, controlled the speed at 400r / min, and then added polyethylene glycol 0.8 g, 2.88g of anhydrous sodium acetate, the mixture continued to stir for 20min, and formed a yellow-brown liquid after mutual dissolution, transferred the liquid into a polytetrafluoroethylene reactor and sealed it, an...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
control rate | aaaaa | aaaaa |
control rate | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com