Device and method for testing leveling property of solid propellant slurry
A solid propellant and testing device technology, which is applied in measurement devices, flow characteristics, instruments, etc., can solve the problems of easy generation of holes or other defects, affecting the structural integrity of the grain column, and poor leveling performance of the slurry, etc. The effect of small error, novel design and simple structure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] Embodiment 1 Butylated hydroxy propellant slurry leveling test
[0049] Before the test, adjust the position of the central piston 6 to the lowest end by rotating the transmission shaft 1, turn on the power supply of the constant temperature circulating water tank 2, adjust the temperature setting value on the constant temperature circulating water tank 2, and inject the constant temperature water into the sample insulation sleeve through the guide tube 3 8. Form a water circulation through the guide tube 3, so that the temperature of the circulating water in the sample insulation sleeve 8 is the same as the temperature of the slurry;
[0050] Extract the slurry with a sampler, squeeze the slurry into the clean sample pool 7, until the surface of the slurry is flush with the upper end of the dial 5, and cover the heat preservation cover 9;
[0051] After the slurry is installed, the connecting rod 12 is driven to swing by rotating the transmission shaft 1, and the cen...
Embodiment 2
[0055] Embodiment 2 Butylated hydroxy propellant leveling test, formula is the same as embodiment 1
[0056] Before the test, adjust the position of the central piston 6 to the lowest end by rotating the transmission shaft 1, turn on the power supply of the constant temperature circulating water tank 2, adjust the temperature setting value on the constant temperature circulating water tank 2, and inject the constant temperature water into the sample insulation sleeve 8 through the guide tube , the water circulation is formed through the guide tube 3, so that the temperature of the circulating water in the sample insulation sleeve 8 is the same as the temperature of the slurry;
[0057] Extract the slurry with a sampler, squeeze the slurry into the clean sample pool 7, until the surface of the slurry is flush with the upper end of the dial 5, and cover the heat preservation cover 9;
[0058] After the slurry is installed, the connecting rod 12 is driven to swing by rotating t...
Embodiment 3
[0062] Embodiment 3 Azide polyether propellant leveling test
[0063] Before the test, adjust the position of the central piston 6 to the lowest end by rotating the transmission shaft 1, turn on the power supply of the constant temperature circulating water tank 2, adjust the temperature setting value on the constant temperature circulating water tank 2, and inject the constant temperature water into the sample insulation sleeve 8 through the guide tube , the water circulation is formed through the guide tube 3, so that the temperature of the circulating water in the sample insulation sleeve 8 is the same as the temperature of the slurry;
[0064] Extract the slurry with a sampler, squeeze the slurry into the clean sample pool 7, until the surface of the slurry is flush with the upper end of the dial 5, and cover the heat preservation cover 9;
[0065] After the slurry is installed, the connecting rod 12 is driven to swing by rotating the transmission shaft, and the central ...
PUM