Embodiment 1
[0016] Embodiment 1, an art type powder coating, comprises the following components by weight, 60 parts of polyester resin, 20 parts of epoxy resin, 30 parts of filler, 1 part of leveling agent, 2 parts of accelerator, incompatible 1 part of polymer, 0.5 part of draping agent, 0.3 part of polyethylene wax, and 0.2 part of carbon black. Among them, the filler is titanium dioxide, the leveling agent is PV-88 leveling agent, and the accelerator is 32-18A accelerator.
Embodiment 2
[0017] Embodiment 2, an art type powder coating, comprises the following components by weight, 70 parts of polyester resin, 25 parts of epoxy resin, 35 parts of filler, 2 parts of leveling agent, 3 parts of accelerator, incompatible 2 parts of polymer, 1.0 part of draping agent, 0.4 part of polyethylene wax, and 0.3 part of carbon black. Among them, the filler is titanium dioxide, the leveling agent is PV-88 leveling agent, and the accelerator is 32-18A accelerator.
Embodiment 3
[0018] Embodiment 3, a kind of artistic type powder coating, comprises the following components by weight, 80 parts of polyester resins, 30 parts of epoxy resins, 40 parts of fillers, 3 parts of leveling agents, 5 parts of accelerators, incompatible 3 parts of polymer, 1.5 parts of draping agent, 0.5 parts of polyethylene wax, and 0.5 parts of carbon black. Among them, the filler is titanium dioxide, the leveling agent is PV-88 leveling agent, and the accelerator is 32-18A accelerator.
[0019] A kind of preparation method of artistic type powder coating, comprises the following steps,
[0020] S1: Take polyester resin, epoxy resin, filler, leveling agent, accelerator, incompatible polymer, drooping agent, polyethylene wax, carbon black in parts by weight, and put them into a mixer and mix them evenly. Time 5-8 minutes;
[0021] S2: Put the mixture in S1 into the extruder to melt, the extrusion temperature is 120°C-150°C, and the time is 30-60 minutes;
[0022] S3: Compress...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com