Anti-corrosion anti-cracking permeability reducing agent for marine concrete and preparation method of anti-corrosion anti-cracking permeability reducing agent

A marine concrete and penetrating agent technology, applied in the field of concrete admixture, can solve the problems of corrosion of steel bars and metal embedded parts, affecting the durability of concrete, and being easily leached by erosive solutions, so as to prolong the service life, improve durability, The effect of improving the corrosion resistance

Active Publication Date: 2022-06-17
日照海工研新材料有限公司
View PDF10 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

However, some waterproof admixtures containing chloride ions are likely to aggravate the corrosion of steel bars and metal embedded parts inside the concrete; waterproofing agents containing expansion components, if the early maintenance conditions of the concrete are not good, and the early expansion value of the expansion agent is too large, it is easy to cause late concrete corrosion. Cracking affects the anti-corrosion effect; admixtures containing fatty acids can form a hydrophobic layer inside the concrete, and there are hydrophobic substances in the capillary pores of the concrete, but in the case of long-term aggressive solution erosion, the effective components The bond between the concrete matrix and the degradation is easy to be leached by the erosive solution, which affects the durability of concrete

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Anti-corrosion anti-cracking permeability reducing agent for marine concrete and preparation method of anti-corrosion anti-cracking permeability reducing agent

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] An anti-corrosion, anti-cracking, and permeability-reducing agent for marine concrete, comprising the following parts by weight of raw materials: 5 parts of water reducing agent, 4 parts of micro-nano anti-permeability components, 1.5 parts of air-entraining agent, 3 parts of anti-cracking fibers, 1 part of phytate, 1 part of polypropylene alcohol, 0.5 part of hydroxypropyl distarch phosphate, 0.5 part of chitosan, and 20 parts of water.

[0028] The water reducing agent is sodium methylnaphthalene sulfonate water reducing agent.

[0029] The preparation method of the micro-nano impermeable component is as follows: immersing the nano-silicon dioxide in a sulfuric acid solution with a mass concentration of 30% according to a solid-to-liquid ratio of 1g:10ml, and then adding coconut oil fatty acid diethanol with a mass of 1% of the mixed solution. amide, stirred and heated in a water bath for 1 hour at 60-70 °C, then added 10% of the mass of the mixed liquid redispersible...

Embodiment 2

[0037] An anti-corrosion, anti-cracking, and permeability-reducing agent for marine concrete, comprising the following parts by weight of raw materials: 7 parts of water reducing agent, 6 parts of micro-nano anti-permeability components, 2 parts of air-entraining agent, 5 parts of anti-cracking fibers, 2 parts of phytate, 2 parts of polypropylene alcohol, 0.8 part of hydroxypropyl distarch phosphate, 1 part of chitosan, and 25 parts of water.

[0038] The water reducing agent is a sulfamate water reducing agent.

[0039]The preparation method of the micro-nano impermeable component is as follows: the nano-silicon dioxide is soaked in a sulfuric acid solution with a mass concentration of 35% according to a solid-to-liquid ratio of 1g:15ml, and then the coconut oil fatty acid diethanol of 2% by mass of the mixed solution is added. amide, stirred and heated in a water bath for 1.5 hours at 60-70 °C, and then added 15% of the mass of the mixed liquid redispersible latex powder and...

Embodiment 3

[0047] An anti-corrosion, anti-cracking and permeability-reducing agent for marine concrete is prepared from the following raw materials in parts by weight: 8 parts of water reducing agent, 8 parts of micro-nano anti-permeability components, 3 parts of air-entraining agent, 7 parts of anti-cracking fibers, 2 parts of phytate, 4 parts of polypropylene alcohol, 0.7 parts of hydroxypropyl distarch phosphate, 1.2 parts of chitosan, and 25 parts of water.

[0048] The water reducing agent is an aliphatic water reducing agent.

[0049] The preparation method of the micro-nano impermeable component is as follows: the nano-silicon dioxide is soaked in a sulfuric acid solution with a mass concentration of 40% according to a solid-to-liquid ratio of 1g:20ml, and then the coconut oil fatty acid diethanol with a mass concentration of 3% of the mixed solution is added. amide, stir and heat in a water bath for 2 hours at 60-70°C, then add 20% of redispersible latex powder and 1% of fatty al...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an anti-corrosion anti-cracking permeability reducing agent for marine concrete and a preparation method of the anti-corrosion anti-cracking permeability reducing agent, and belongs to the technical field of concrete admixtures. The anti-seepage agent is prepared from the following raw materials in parts by weight: 5 to 10 parts of a water reducing agent, 4 to 10 parts of a micro-nano anti-seepage component, 1.5 to 3.5 parts of an air entraining agent, 3 to 9 parts of anti-crack fiber, 1 to 3 parts of inositol hexaphosphate, 1 to 5 parts of polypropylene glycol, 0.5 to 1 part of hydroxy propyl distarch phosphate, 0.5 to 1.5 parts of chitosan and 20 to 30 parts of water. According to the anti-seepage agent disclosed by the invention, nano silicon dioxide is modified in two steps and then is mixed with the anti-cracking fiber, two isolated strength enhancing substances are organically combined and jointly act with other raw materials, the anti-seepage and anti-cracking properties of a concrete material are remarkably improved, and the obtained admixture does not contain substances harmful to a human body, is chlorine-free, green and environment-friendly, and has a good application prospect. The durability of the concrete in the marine environment can be greatly improved, the service life is prolonged, and the safety is improved.

Description

technical field [0001] The invention belongs to the technical field of concrete admixtures, and particularly relates to an anti-corrosion, anti-cracking, anti-seepage reducing agent for marine concrete and a preparation method thereof. Background technique [0002] Concrete used in marine engineering, also known as marine concrete. Marine engineering includes coastal engineering and offshore engineering. All structures constructed under the influence of seawater and the concrete used for structures on the shore that are often splashed by waves are all marine concrete. Due to frequent or periodic contact with seawater, the physical and chemical action of seawater or marine atmosphere (containing chloride ions), or the impact and abrasion of waves and running water, marine concrete suffers damage and shortens the service life. In addition to the strength and workability of the mixture, marine concrete should meet the design and construction requirements, and should also have ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C04B24/38C04B20/12C04B20/02C04B103/60C04B103/61C04B103/65C04B14/06
CPCC04B40/0039C04B20/12C04B20/023C04B2103/61C04B2103/65C04B2103/60C04B24/20C04B24/10C04B16/0633C04B24/003C04B24/26C04B24/243C04B24/38C04B14/062C04B2103/302C04B16/0683C04B14/4656C04B20/1025C04B20/1029C04B20/1037Y02W30/91
Inventor 匡利君王忠勇肖维录
Owner 日照海工研新材料有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products