Interior wall inorganic coating prepared from organic-inorganic composite emulsion and preparation method of interior wall inorganic coating
An inorganic composite and inorganic coating technology, which is applied in the direction of fireproof coatings, antifouling/underwater coatings, alkali metal silicate coatings, etc., can solve the problems of poor storage stability and difficult quality control of inorganic coatings, and achieve stable and high chemical properties , fine manufacturing process, the effect of quality improvement
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2022-07-05
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention relates to the technical field of coatings, in particular to an inorganic coating for interior walls prepared from an organic-inorganic composite emulsion and a preparation method thereof. Background technique
[0002] In the field of coatings, compared with the more commonly used water-based organic coatings, water-based inorganic coatings are used in subway tunnels, schools, hospitals, basements because of their more environmentally friendly, non-combustible, self-breathing, antibacterial and anti-mildew properties. It is used in important places with special requirements.
[0003] At present, most of the production technology of inorganic coatings is made of potassium silicate, lithium silicate, silica sol or one of these materials and organic emulsions as adhesive materials, and adding appropriate amount of pigments and fillers, water-based coating additives. However, the disadvantage of this formula is that the inorganic adhesive ma...
Examples
preparation example Construction
[0067] The present invention also provides a method for preparing an inorganic coating for interior walls made of the above-mentioned organic-inorganic composite emulsion, characterized in that it includes the following steps:
[0068] S100, first mixing water and bactericide to obtain a first mixed solution;
[0069] S200, carrying out the second mixing of the powdery thickener and the first mixed solution to obtain the second mixed solution;
[0070] S300, performing a third mixing of the dispersant, the defoaming agent, and the second mixed solution to obtain a third mixed solution;
[0071] S400, performing a fourth mixing with the pH regulator and the third mixed solution to obtain a fourth mixed solution;
[0072] S500, carrying out the fifth mixing of the defoaming agent and the fourth mixed solution to obtain the fifth mixed solution;
[0073] S600, carrying out sixth mixing of titanium dioxide, kaolin, functional filler and the fifth mixed solution to obtain a sixth...
Embodiment 1
[0086] A raw material preparation (total 100g): water 18g, powdery thickener 0.2g, bactericide 0.1g, dispersant 0.4g, wetting agent 0.1g, defoamer 0.7g, pH adjuster 0.1g, titanium dioxide 20g, 3g kaolin, 22.4g functional filler, 35g organic-inorganic composite emulsion.
[0087] B. Preparation of inorganic coatings for interior walls:
[0088] 1) Use deionized water for high-speed dispersion kettle 1, low-speed paint-adjusting kettle 2, powder transportation pipeline 3, water transportation pipeline 4, high-speed dispersion process liquid auxiliary raw material transportation pipeline 5, water slurry delivery pipeline 6, The liquid raw material conveying pipeline 7, the organic-inorganic composite emulsion conveying pipeline 8, and the finished product unpacking pipeline 9 in the paint mixing process are cleaned up, and the excess polyvalent ion impurities are taken out;
[0089] 2) Add deionized water to the high-speed dispersing kettle 1 through the water delivery pipeline ...
Embodiment 2
[0097] A raw material preparation (total 100g): water 25g, powdery thickener 0.5g, bactericide 0.15g, dispersant 0.6g, wetting agent 0.15g, defoamer 0.45g, pH adjuster 0.15g, titanium dioxide 15g, 5g kaolin, 28g functional filler, 25g organic-inorganic composite emulsion.
[0098] B. Preparation of inorganic coatings for interior walls:
[0099]1) Use deionized water for high-speed dispersion kettle 1, low-speed paint-adjusting kettle 2, powder transportation pipeline 3, water transportation pipeline 4, high-speed dispersion process liquid auxiliary raw material transportation pipeline 5, water slurry delivery pipeline 6, The liquid raw material conveying pipeline 7, the organic-inorganic composite emulsion conveying pipeline 8, and the finished product unpacking pipeline 9 in the paint mixing process are cleaned up, and the excess polyvalent ion impurities are taken out;
[0100] 2) Add deionized water to the high-speed dispersing kettle 1 through the water delivery pipeline...