Processing method of whole cotton non-ironimg face fabric
A processing method and fabric technology, applied in textiles and papermaking, fiber treatment, plant fibers, etc., can solve problems affecting product quality, temperature difference between the edge of the cloth surface and the head and tail, performance differences, etc., to avoid excessive damage to the fabric, Reduce formaldehyde content and meet the effect of clothing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Embodiment 1: A processing method for pure cotton non-ironing fabrics, the technological process is as follows: ① singeing, clean singeing is required; ② desizing, clean desizing is required, and the desizing rate reaches more than 98%; ③ mercerizing , requires sufficient mercerization, and the pH value of the fabric is about 7; ④Resin is applied, the drying temperature is 90°C, the temperature of the cloth surface is 35°C, the moisture content is 6%, and the pH value of the resin mixture is 1; After the resin is shaped and packaged, it is rewound in a constant temperature room at 35°C. The temperature of the fabric surface after rewinding is 40°C; Place for 20 hours; ⑦Alkaline washing, using soda ash solution at room temperature of 23°C, the pH value of the soda ash solution is 10; ⑧Washing, use clear water at a water temperature of 70°C; ℃, the pressure is 160N / mm 2 ;Finally preshrunk.
Embodiment 2
[0019] Embodiment 2: A processing method of a pure cotton non-ironing fabric, the technological process is as follows: 1. singeing, clean singeing is required; 2. desizing, clean desizing is required, and the desizing rate reaches more than 98%; 3. mercerizing , requires sufficient mercerization, and the pH value of the fabric is about 7; ④ resin, the drying temperature is 80 ° C, the temperature of the cloth surface is 45 ° C, the moisture content is 8%, and the pH value of the resin mixture is 4; After the resin is shaped and packaged, it is rewound in a constant temperature room at 40°C. The temperature of the fabric surface after rewinding is 35°C; Place for 14 hours; ⑦Alkali washing, using soda ash solution at room temperature of 23°C, the pH value of the soda ash solution is 11; ⑧Washing, use clear water at a water temperature of 70°C; ℃, the pressure is 180N / mm 2 ;Finally preshrunk.
Embodiment 3
[0020] Embodiment three: a kind of processing method of pure cotton non-ironing fabric, its technological process is as follows in order: ① singeing, require to achieve singeing clean; ② desizing, require desizing to be clean, desizing rate reaches more than 98%; , requires sufficient mercerization, and the pH value of the fabric is about 7; ④ For resin, the drying temperature is 100 ° C, the temperature of the cloth surface is 25 ° C, the moisture content is 5%, and the pH value of the resin mixture is 1; After the resin is shaped and packaged, it is rewound in a constant temperature room at 30°C. The temperature of the fabric surface after rewinding is 30°C; Place for 24 hours; ⑦Alkaline washing, using soda ash solution at room temperature of 23°C, the pH value of the soda ash solution is 10; ⑧Washing, use clear water at a water temperature of 70°C; ℃, the pressure is 130N / mm 2 ;Finally preshrunk.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com