Main charging composition for focus explosive pillar an dits production process
A technology of seismic source charge column and main charge, which is applied to explosives and other directions, can solve the problems of high physical harm to operators, high TNT content and high production cost, and achieve the effects of reducing physical harm, less environmental pollution, and high degree of safety.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0012] A main charge formula of a seismic source powder column, the content of each component is by weight TNT: ammonium nitrate: wood flour: organic or inorganic surface modifier = 25-40: 60-70: 0-5: 0-2 , the organic or inorganic surface modifying agent is one or more of them in any proportion mixture of paraffin wax, fluorine-containing surfactant or graphite. Fluorosurfactant is CnF (2n+1) COOM, where n is 8-13, M is Li + 、Na + , NH4 + 、H + .
[0013] A kind of main charge production technology of seismic source powder column, will by weight TNT: ammonium nitrate: wood flour: organic or inorganic surface modifier=25-40: 60-70: 0-5: 0-2 in the formula Add each component in any order to an open rotary plasticizing pot, mix and plasticize at a temperature of 81--90°C for 10-25 minutes.
PUM
Property | Measurement | Unit |
---|---|---|
density | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com