Embodiment 1
[0013] (1), plate preparation: the basic density is lower than 0.55g / cm 3 Fresh or high-humidity low-density fast-growing eucalyptus is processed into various specifications of boards suitable for construction;
[0014] (2) Intermittent drying of wood: put the board into the drying kiln, and use a temperature of 80°C and a humidity of 90 to keep it for 1 hour-a temperature of 15°C and a humidity of 90% to keep it for 4 hours in multiple intermittent cycles. Dry to a moisture content of about 30% to stop the batch process;
[0015] (3), and then use the drying process based on the kiln drying standard of the Baidu test method to dry the wood to the required equilibrium moisture content, which can reduce the shrinkage rate of eucalyptus wood to less than 5%, and other physical and mechanical indicators have reached the national level. standard requirements.
Embodiment 2
[0017] (1), plate preparation: the basic density is lower than 0.55g / cm 3 Fresh or high-humidity low-density fast-growing eucalyptus is processed into various specifications of boards suitable for furniture;
[0018] (2), wood intermittent drying: put the board into the drying kiln, adopt a temperature of 90°C and a humidity of 90% to keep for 4 hours - a temperature of 25°C and a humidity of 95% to keep for 1 hour in multiple intermittent cycles. The wood is dried to a moisture content of about 35% to stop the batch process;
[0019] (3), and then adopt the conventional kiln drying process to dry the wood to the required equilibrium moisture content, which can reduce the shrinkage rate of the eucalyptus wood to less than 10%, and other physical and mechanical indexes all meet the requirements of the national standard.
Embodiment 3
[0021] (1), plate preparation: the basic density is lower than 0.55g / cm 3 The fresh or high-humidity low-density fast-growing eucalyptus is processed into various specifications boards suitable for interior decoration;
[0022] (2) Intermittent drying of wood: put the board into a conventional drying kiln, and use a temperature of 100°C and a humidity of 100% to keep it for 6 hours-a temperature of 30°C and a humidity of 100% for 2 hours. Dry the wood until the moisture content is about 40% to stop the batch process;
[0023] (3) Then, the conventional kiln drying process is used to dry the wood to the required equilibrium moisture content, which can reduce the shrinkage rate of the eucalyptus wood to less than 4%, and other physical and mechanical indexes all meet the requirements of the national standard.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com