A technology for water fracturing and oil and gas wells, which is applied in earthwork drilling, wellbore/well components, sealing/isolation, etc., and can solve the problem of not being able to effectively avoid oil well flooding, not being able to effectively prevent bottom water from coning into the wellbore, and diverting agent or temporary plugging agent settling speed is slow to achieve the effect of preventing flooding
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0042] 1. After heating and melting 200Kg50# paraffin in the coating machine, add 1800Kg of quartz sand to the melted paraffin and cool down, and form a coating proppant in the coating machine;
[0043] 2. Add 9817Kg of water into the container with pump circulation or agitator, then turn on the pump circulation or agitator, slowly add 35Kg of low molecular weight thickener, then add 100Kg of clay stabilizer, 10Kg of crude oil demulsifier, 5Kg of surface active agent, 3KgpH regulator, 30Kg bactericide, and then continue to circulate or stir for 30 minutes to make the liquid mix evenly and form a mixed solution;
[0044] 3. Mix the mixed solution and the cross-linking agent again according to the volume ratio of 100:0.7 to form a pre-gel solution.
[0045] 4. Mix the jelly pre-fluid and the coated proppant at a weight ratio of 100:30, stir evenly, and pump them into the destination layer.
Embodiment 2
[0047] 1. After heating and melting 200Kg60# paraffin in the coating machine, add 18000Kg of quartz sand to the melted paraffin and cool down, and form a coating proppant in the coating machine;
[0048] 2. Add 9817Kg of water into the container with pump circulation or agitator, then turn on the pump circulation or agitator, slowly add 35Kg of low molecular weight thickener, then add 100Kg of clay stabilizer, 10Kg of crude oil demulsifier, 5Kg of surface active agent, 3KgpH regulator, 30Kg bactericide, and then continue to circulate or stir for 30 minutes to make the liquid mix evenly and form a mixed solution;
[0049] 3. Mix the mixed solution and the cross-linking agent again according to the volume ratio of 100:0.7 to form a pre-gel solution.
[0050] 4. Mix the jelly pre-fluid and the coated proppant at a weight ratio of 100:30, stir evenly, and pump them into the destination layer
Embodiment 3
[0052] 1. After heating and melting 300Kg70# paraffin in the coating machine, add 1700Kg of quartz sand to the melted paraffin and cool down to form a coating proppant in the coating machine;
[0053] 2. Add 9811Kg of water into the container with pump circulation or agitator, then turn on the pump circulation or agitator, slowly add 40Kg of low molecular weight thickener, then add 100Kg of clay stabilizer, 10Kg of crude oil demulsifier, 5Kg of surface active agent, 4KgpH regulator, 30Kg bactericide, and then continue to circulate or stir for 30 minutes to make the liquid mix evenly and form a mixed solution;
[0054] 3. Mix the mixed solution and the cross-linking agent again according to the volume ratio of 100:0.7 to form a pre-gel solution.
[0055] 4. Mix the jelly pre-fluid and the coated proppant at a weight ratio of 100:30, stir evenly, and pump them into the destination layer