Grave protection material and preparation thereof
A technology of protective materials and tombs, which is applied in the field of preparation of the protective materials, can solve the problems of ashes damage, difficulty in safety of the deceased, and affecting the preservation of ashes, and achieve the effect of preventing decay and lasting effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Material selection: There are many types of attapulgite clay. Attapulgite clay with good adsorption and bonding properties should be selected. Visible miscellaneous stones and other foreign objects should be removed, and it should be allowed to weather naturally for 40 days to continuously disintegrate into smaller non-clay particles. Regular lumps, and air-dried, the moisture should be ≤ 12%, the alum is selected from better quality crystalline alum, the gypsum is anhydrite, cloves and natural spices are selected from better quality, and the moisture should be ≤ 10%. Quicklime, boric acid, copper sulfate, realgar and activated carbon meet industry standards.
[0025] Ingredients: Group A ingredients: 62.5 kg of attapulgite clay, 5 kg of quicklime, 2.4 kg of alum, 4.3 kg of activated carbon and 2.8 kg of gypsum. Group B ingredients: 14.5 kg of attapulgite clay, 6.1 kg of boric acid, 2.4 kg of realgar, 4.6 kg of copper sulfate, 2.8 kg of cloves, 2.6 kg of natural spices,...
Embodiment 2
[0032] Material selection: same as Example 1.
[0033] Ingredients: Group A ingredients: 56 kg of attapulgite clay, 4.9 kg of quicklime, 2.1 kg of alum, 4.2 kg of activated carbon and 2.8 kg of gypsum. Group B ingredients: 12 kg of attapulgite clay, 6 kg of boric acid, 2.4 kg of realgar, 4.5 kg of copper sulfate, 2.7 kg of cloves, 2.4 kg of natural spices, including 1.2 kg each of sandalwood and Wujiapi.
[0034] Grinding: with embodiment 1.
[0035] Finished product: After grinding, the weight of group A is 70 kg; the weight of group B is 27.6 kg; after cooling of group B, realgar powder is added, mixed evenly with a mixer to form a finished product, and the weight of the finished product is 100 kg.
[0036] The proportioning of various materials in Examples 3-9 is shown in Table 1, and the preparation method and process are the same as in Example 1.
[0037] Table 1 (unit: kg)