A technology with high wear resistance and manufacturing method, which is applied in the direction of manufacturing tools, arc welding equipment, mechanical equipment, etc., can solve the problems of poor surface carburizing and quenching process, difficulty in meeting process requirements, high hardness of contact surface, etc., and achieve wear resistance Good performance, easy to popularize, and guarantee the effect of wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Embodiment 1: A high wear-resistant skateboard seat, the sliding surface of the high wear-resistant skateboard seat is provided with 4 grooves keeping a certain distance from each other along the arc direction of the sliding surface, and the 4 grooves are The grooves are evenly distributed, and the arrangement direction of the grooves is consistent with the direction of the center line of the arc surface of the sliding surface. The grooves are filled with hard steel fillers. The cross-section of the grooves is semicircular, and the diameter of the semicircle is φ10.
Embodiment 2
[0021] Embodiment 2: A high wear-resistant skateboard seat, the sliding surface of the high wear-resistant skateboard seat is provided with 6 grooves keeping a certain distance from each other along the arc direction of the sliding surface, and the 6 grooves are Evenly distributed, the arrangement direction of the groove is consistent with the direction of the center line of the arc surface of the sliding surface, the groove is filled with hard steel filler, the cross section of the groove is semicircular, and the diameter of the semicircle is φ12.
[0022] As a transformation of the first and second embodiments above, the number of grooves can be determined according to needs, generally 4-12; The diameter is generally between φ10~φ12; the shape of the cross section of the groove can also be other shapes, such as arc or inverted trapezoid or inverted triangle, etc. The depth and width of the groove are generally controlled within the semicircle of the groove with a semicircular...
Embodiment 3
[0023] Embodiment 3: A method for manufacturing a highly wear-resistant skateboard seat, the method includes the following steps:
[0024] A. Pre-casting groove: when casting the skateboard seat, grooves are pre-cast on the sliding surface of the skateboard seat and along the arc direction of the sliding surface according to the required number and shape;
[0025] B. Groove surface treatment: Shot peening the groove surface to eliminate casting stress and clean impurities on the groove surface at the same time;
[0026] C. Preheating of the welding substrate: preheat the welding substrate of the sliding seat to 130°C;
[0027] D. Overlay welding groove: use EDPCrMo-A4-03 electrode that meets the requirements of GB / T 984-1985, use manual arc welding machine welding to apply hard steel electrode surfacing welding to the groove, welding voltage is 70V, electrode surfacing current Take 200A to fill the groove with hard steel filler, and the hardness of the surfacing layer meets t...