Water soluble environment-friendly coating for inner wall and preparation method thereof
An environmentally friendly paint, water-soluble technology, applied in the field of interior wall paint, to achieve the effect of short drying time and good adhesion
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] (1) 180 kg of pure water, 3 kg of acid vinegar, and 9 kg of glycerin are put into the kettle and stirred evenly;
[0023] (2) keep stirring, put 8 kg of chitosan and 3 kg of polyvinylpyrrolidone into the kettle and heat at 30°C to 80°C (gradually warming up) to stir for 0.5 to 3 hours;
[0024] (3) Keep stirring and put 80 kg of kaolin, 20 kg of titanium dioxide, and 10 kg of silicon dioxide into the kettle one by one and stir for 2 to 3 hours;
[0025] (4) When all the above materials are mixed evenly, stop the machine and mature for 12 to 36 hours;
[0026] (5) Measure the product index and adjust it to the theoretical value;
[0027] (6) After stirring slowly for half an hour, cool, weigh and pack.
Embodiment 2
[0029] A kind of preparation method for the water-soluble environment-friendly paint of interior wall, this method comprises the following steps:
[0030] (1) 55 kilograms of purified water, 3 kilograms of acetic acid, and 3 kilograms of glycerin are dropped into the kettle by weight and stirred;
[0031] (2) Keep stirring and put 3 kg of chitosan and 3 kg of polyvinylpyrrolidone into the reaction kettle in turn, heat up from 30°C to 80°C, and stir for 0.3 to 1 hour;
[0032] (3) After being fully mixed, add 20 kg of kaolin, 7 bases of titanium dioxide, and 5 kg of silicon dioxide into the kettle gradually, keep stirring at 600 rpm for 3 hours;
[0033] (4) After mixing evenly, gradually reduce the rotating speed, shut down and mature for 12 to 36 hours to obtain the mixture;
[0034] (5) the solid content of the mixture obtained in the measurement step (4) is 30%, which meets the product requirements;
[0035] (6) Stir slowly for 0.3 to 1 hour and cool to obtain the product...
Embodiment 3
[0037] A kind of preparation method for the water-soluble environment-friendly paint of interior wall, this method comprises the following steps:
[0038] (1) 65 kilograms of purified water, 1 kilogram of acetic acid, and 1 kilogram of glycerin are dropped into the kettle by weight and stirred;
[0039] (2) Keep stirring and put 0.8 kg of chitosan and 0.5 kg of polyvinylpyrrolidone into the reaction kettle in turn, heat up from 30°C to 80°C, and stir for 1 to 1.5 hours;
[0040] (3) After fully mixing, add 30 kg of kaolin, 4 kg of titanium dioxide, and 1 kg of silicon dioxide into the kettle gradually, keep stirring at 1000 rpm for 2 hours;
[0041] (4) After mixing evenly, gradually reduce the rotating speed, shut down and mature for 12 to 36 hours to obtain the mixture;
[0042] (5) the solid content of the mixture obtained in the measurement step (4) is 35%, which meets the product requirements;
[0043] (6) Stir slowly for 0.3 to 1 hour and cool to obtain the product.