Production method of Chengni inkstone with Xi glaze
A production method and technology of inkstone, applied in the production field of Xiglacheng mud inkstone, can solve the problems that the color of inkstone cannot be controlled artificially, and the production method of Chengni inkstone is lost, so as to protect the precious folk cultural heritage, fine texture, and promote traditional crafts Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment Construction
[0007] A production method of the glaze clear mud inkstone includes the following steps: (a) drying the ancient sediment from the Hutuo River in Wutai County, Shanxi Province; (b) putting the dried ancient sediment in the water Add water to the tank and soak for two hours; (c) Stir the soaked ancient sediment into mud; (d) Filter the mud; (e) Knead and beat the filtered mud to form a mud mass; (f) ) Put the mud mass into the mold to make a blank; (g) Put the blank into the refractory box, and put the refractory box into the kiln. The temperature of the kiln is controlled at 980℃~1050℃, and the kiln temperature is controlled at 980℃~1050℃, firing for 72 hours to obtain the Chengmu inkstone; (H) Put the Chengni inkstone into the smoker to smoke. The smoked material is made by mixing 5kg of millet bran and rice bran each. After the smoked material is burned, the glaze clear mud inkstone is obtained. The filtration in step (d) is carried out in two steps, the first step is filtrati...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More