Method for recycling titanium from sulfuric acid method titanium white acidolysis residue

A technology of titanium dioxide acidolysis residue and sulfuric acid method, which is applied in chemical instruments and methods, wet separation, solid separation, etc., can solve problems such as environmental hazards, waste of valuable resources, and reduction of corporate profits, so as to protect the environment and solve Effects of potential harm and huge social benefits

Inactive Publication Date: 2012-11-07
云南昆欧科技有限责任公司
View PDF2 Cites 9 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Because these waste residues are the products of sulfuric acid soaking process, the surface characteristics have changed greatly. So far, the comprehensive utilization and recycling of black waste residues have not been well resolved, and they are basically treated as waste. Disposal, which not only wastes the valuable resources and reduces the profit of the enterprise, but also the discharge of acid waste piles will cause harm to the local environment

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment Construction

[0012] The content of the present invention is further described below in conjunction with the embodiments.

[0013] A method for recycling titanium from acid hydrolysis residues of titanium dioxide by sulfuric acid method, characterized in that the production method is as follows:

[0014] ①Wash the acid hydrolysis residue of titanium dioxide produced by sulfuric acid method, and use a cyclone to remove the fine mud in the residue;

[0015] ② Prepare the slurry, the concentration of the slurry is 20-30%, and adjust the pH value of the slurry with oxalic acid, and the pH value of the end point is 6-7;

[0016] ③Add 2# oil as a foaming agent, ROB as a collector, and control the temperature to be 20-40 °C for two-stage flotation to obtain titanium ore, which is dried for the production of titanium dioxide; the recovered titanium ore grade is >46% , the recovery rate> 85%.

[0017] The process parameter index of the float selection production in the present invention is: the p...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a method for recycling titanium from sulfuric acid method titanium white acidolysis residue. The method comprises the following steps of: (1) washing the acidolysis residue produced when titanium white powder is produced by using a sulfuric acid method, and removing fine silt from the residue by using a cyclone; (2) preparing residue pulp of which the concentration is 20 to 30 percent, and regulating the pH of the residue pulp by using oxalic acid, wherein the final pH value is 6 to 7; and (3) adding No.2 oil serving as a foaming agent and ROB serving as a collecting agent, controlling the temperature to be between 20 and 40 DEG C, performing two-stage flotation to obtain titanium ore, drying, and thus obtaining a raw material for producing the titanium white powder, wherein the grade of the recovered titanium ore is more than 46 percent, and the recovery rate is more than 85 percent. The method has the advantages of recovering the valuable component in the residue, eliminating potential harm of the stored original acidolysis residue to the environment, protecting the environment and bringing huge social benefits.

Description

technical field [0001] The invention relates to the technical field of recycling titanium from the acidolysis residue of producing titanium dioxide by a sulfuric acid method. Background technique [0002] There are two kinds of titanium dioxide production: sulfuric acid method and chlorination method. my country's titanium dioxide production mainly adopts sulfuric acid method. For every ton of titanium dioxide produced, in addition to producing 8-10 tons of dilute sulfuric acid and 3-3.5 tons of ferrous sulfate heptahydrate , but also to discharge 0.2 to 0.3 tons of insoluble black waste residue. Analysis shows that the content of titanium dioxide in these waste residues is about 25%, which has recycling value. Since these waste residues are the products of the sulfuric acid soaking process, the surface characteristics have changed greatly. So far, the comprehensive utilization and resource treatment of black waste residues have not been well resolved, and they are basically...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): B03B7/00
Inventor 蒋朋钢
Owner 云南昆欧科技有限责任公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products