Traceless washing-free wax solvent for vehicle
A scrub-free, wax-water-free technology, applied in detergent compositions, soap detergent compositions, surface-active non-soap compounds and washing compositions, etc., can solve red, swollen, cracked and long-standing frostbite of hands, lack of quality assurance in car washing, Scrubbing can not be well standardized to achieve the effect of solving incomplete cleaning, saving labor costs and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] 1. First dissolve 1Kg of palm wax with 3Kg of acetone, then put it into the reaction kettle and heat it to 50°C, then add 5Kg of surfactant AES and 1Kg of fatty alcohol polyoxyethylene ether AEO-9 to fully dissolve it.
[0025] 2. Dissolve 3Kg sodium tripolyphosphate into 10Kg hydrofluoric acid, and then dissolve 3Kg alkylphenol polyoxyethylene ether TX-10 into the above-mentioned mixed solution of sodium tripolyphosphate and hydrofluoric acid.
[0026] 3. Mix the mixture prepared in step 1 and step 2 and stir thoroughly for 30 minutes. After the mixture is completely fused, add 5Kg sodium silicate, 1Kg sodium chloride, 0.3Kg pigment and 0.3Kg essence in sequence and stir fully Leave to stand after 30 minutes;
[0027] 4. Let it stand for two hours to eliminate the foam and fill it into a finished product. The finished product is diluted with water at a ratio of 1:100 before use.
Embodiment 2
[0029] 1. First dissolve 3Kg of palm wax with 5Kg of acetone, then put it into the reaction kettle and heat it to 50°C, then add 8Kg of surfactant AES and 3Kg of fatty alcohol polyoxyethylene ether AEO-9 to fully dissolve it.
[0030] 2. Dissolve 5Kg sodium tripolyphosphate into 15Kg hydrofluoric acid, and then dissolve 5Kg alkylphenol polyoxyethylene ether TX-10 into the mixed solution of sodium tripolyphosphate and hydrofluoric acid.
[0031] 3. Mix the mixture prepared in step 1 and step 2 and stir thoroughly for 30 minutes. After the mixture is completely fused, add 8Kg sodium silicate, 3Kg sodium chloride, 0.2Kg pigment and 0.4Kg essence in turn and stir fully Leave to stand after 30 minutes;
[0032] 4. Let it stand for two hours to eliminate the foam and fill it into a finished product. The finished product is diluted with water at a ratio of 1:100 before use.
Embodiment 3
[0034] 1. First dissolve 5Kg of palm wax with 8Kg of acetone, then put it into the reactor and heat it to 50°C, then add 10Kg of surfactant AES and 5Kg of fatty alcohol polyoxyethylene ether AEO-9 to fully dissolve it.
[0035] 2. Dissolve 8Kg of sodium tripolyphosphate into 20Kg of hydrofluoric acid, and then dissolve 8Kg of alkylphenol polyoxyethylene ether TX-10 into the above-mentioned mixed solution of sodium tripolyphosphate and hydrofluoric acid.
[0036] 3. Mix the mixture prepared in step 1 and step 2 and stir thoroughly for 30 minutes. After the mixture is completely fused, add 10Kg sodium silicate, 5Kg sodium chloride, 0.5Kg pigment and 0.5Kg essence in turn and stir fully Leave to stand after 30 minutes;
[0037] 4. Let it stand for two hours to eliminate the foam and fill it into a finished product. The finished product is diluted with water at a ratio of 1:100 before use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com