Embodiment 1
[0040] Embodiment 1 blue-green fountain cold fireworks
[0041] The formula used is: ① Ammonium perchlorate 30%, ② Nitrocellulose 20%, ③ Silver titanium powder 30%, ④ Guangzhou Tianyu Trading Co., Ltd. TYB-40 blue-green photoluminescent material 15%, ⑤ Fluorine rubber 5% ; Both are mass percentages. The production process is as follows: the first step is to prepare fuel particles, and the process is as follows: firstly mix component ③ with component ④ evenly; then use acetone to dissolve component ⑤ to form a solution; then add the solution of component ⑤ to component ③ ﹑④ in the mixed powder, mixed evenly; the mixture of components ③﹑④﹑⑤ was made into fuel particles with a particle size of 80 mesh by the spheronization method, dried at 50°C, and set aside. The second step is to mix the medicaments, that is to mix the mixed particles of components ①, ② and ③, ④, ⑤ evenly. The third step is to charge the product, and fill the uniformly mixed blue cold smoke into the fountain ...
Embodiment 2
[0043] Embodiment 2 blue fountain cold fireworks
[0044] The formula used is: ① 20% ammonium perchlorate, ② 30% nitrocellulose, ③ 30% silver titanium powder, ④ 15% JC-009 blue photoluminescent material of Shenzhen Jingcheng Arts Co., Ltd., ⑤ 5% fluorine rubber; All are percentages by mass. The production process is as follows: the first step is to prepare fuel particles, and the process is as follows: firstly mix component ③ and component ④ evenly; then use ethyl acetate to dissolve component ⑤ to form a solution; then add the solution of component ⑤ to the component Divide into the mixed powder of ③, ④, and mix evenly; use the extrusion method to make the mixture of components ③, ④, and ⑤ into fuel particles with a particle size of 80 mesh and 40 mesh, dry at 50 ° C, and set aside. The second step is to mix the medicaments, that is to mix the mixed particles of components ①, ② and ③, ④, ⑤ evenly. The third step is to charge the product, and fill the uniformly mixed blue co...
Embodiment 3
[0046] Example 3 Purple Waterfall Cold Fireworks
[0047]The formula used is: ① 20% ammonium perchlorate, ② 20% nitrocellulose, ③ 35% silver titanium powder, ④ 20% zd-9 purple photoluminescent material of Shenzhen Tounao Zhifu Technology Co., Ltd., ⑤ Fluorine rubber 5% %; all are mass percentages. The production process is as follows: the first step is to prepare fuel particles, and the process is as follows: firstly mix component ③ with component ④ evenly; then use acetone to dissolve component ⑤ to form a solution; then add the solution of component ⑤ to component ③ ﹑④ in the mixed powder, mixed evenly; the mixture of components ③﹑④﹑⑤ was made into fuel particles with a particle size of 50 mesh by the spheronization method, dried at 50°C, and set aside. The second step is to mix the medicaments, that is to mix the mixed particles of components ①, ② and ③, ④, ⑤ evenly. The third step is to charge the product, which is to fill the uniformly mixed blue cold smoke into the wat...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com