Normal-pressure dyeing method of fragrant polyester/polyurethane knitting fabric
A technique of dyeing knitted fabrics under normal pressure, which is applied in the dyeing field of polyester-spandex knitted fabrics to achieve the effect of avoiding peculiar smell and toxicity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Example 1: Use Disperse Brilliant Blue E-2BLN 3% (owf) to scratch with 30°C water, then add vanillin 12 g / L, and prepare a dye solution at a bath ratio of 30:1, and use the oil-removed Put the polyester-spandex knitted fabric into the dyeing solution, dye at 95°C for 1 hour, keep warm for 40 minutes for dyeing, then wash twice with hot water at 60°C, and wash with reducing solution composed of 2g / L hydrosulfite and 2g / L soda ash at 50°C After 30 minutes, wash twice with water, heat-set after dehydration. The K / S value of the dyed fabric is 8.135, and the soaping fastness and rubbing fastness are above 4.5.
Embodiment 2
[0018] Example 2: Use 33°C water for marking according to disperse ruby SE-GFL 3% (owf), then prepare a dye liquor with 15 g / L of vanillin at a bath ratio of 40:1, and use the degreased polyester Put the ammonia knitted fabric into the dyeing solution, dye at 90°C for 50 minutes, keep warm for 45 minutes for dyeing, first wash twice with hot water at 60°C, and use a reducing solution composed of 2g / L hydrosulfite and 2g / L soda ash at 50°C for 30 minutes. Wash twice with water, dehydrate and then heat set. The K / S value of the dyed fabric is 7.281, and the soaping fastness and rubbing fastness are above grade 4.5.
Embodiment 3
[0019] Example 3: Marking with 35°C water according to Disperse Red E-3B 2% (owf), then 10 g / L of vanillin, and preparing a dye solution at a bath ratio of 40:1, and the polyester ammonia after degreasing treatment Put the knitted fabric into the dye solution, dye at 90°C for 45 minutes, keep warm for 50 minutes for dyeing, first wash twice with hot water at 60°C, and use a reducing solution composed of 2g / L hydrosulfite and 2g / L soda ash at 50°C for 30 minutes, and then Washed twice, dehydrated and then heat-set. The K / S value of the dyed fabric is 4.998, and the soaping fastness and rubbing fastness are above grade 4.5.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com