Treatment method of waste colloidal emulsion explosive in porous ammonium nitrate fuel oil explosive

A technology of emulsion explosives and ammonium oil explosives, which is applied in the direction of explosives, etc., can solve the problems of high requirements on the surrounding environment, large environmental impact, and difficult implementation, and achieve the effects of overcoming safety and quality hazards, improving the environment, and saving resources

Inactive Publication Date: 2013-09-25
SICHUAN YAHUA IND GRP
View PDF0 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

This method has high requirements on the surrounding environment, requires conditions such as a destruction site, and has a greater impact on the environment. It is becoming more and more difficult to implement it under the current background of building an ecological environment and a harmonious society in the country, and other processing methods are also difficult to achieve.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0029] The ratio of explosive raw materials is in parts by weight

[0030] (1) Put 9 parts of 10# total loss system oil into the melting tank, and then put in 1 part of surfactant, and control the temperature at 100°C;

[0031] (2) Add 10 parts of scrap colloidal emulsion explosive to step (1), which needs to be divided into small pieces and added to the melting tank;

[0032] (3) After adding the materials in step (2), control the temperature at 100°C, keep stirring for 15 minutes, and control the stirring line speed at 6m / s;

[0033] (4) Put 80 parts of porous ammonium nitrate into the mixer, then add the scrap colloidal emulsion explosive mixture pretreated in step (3), keep the temperature, and stir and mix for 5 minutes according to the process regulations;

[0034] (5) Packaging the product prepared in step (4) with a plastic film to obtain a porous ammonium oil explosive;

[0035] The obtained product used 100g of No. 2 rock emulsion explosive as the primer for detona...

Embodiment 2

[0037] The ratio of explosive raw materials is in parts by weight

[0038] (1) Put 4 parts of 10# total loss system oil into the melting tank, then put 2 parts of surfactant, and control the temperature at 100°C;

[0039] (2) Put 34 parts of scrap colloidal emulsion explosives into the melting tank of step (1), and the input needs to be divided into small pieces;

[0040] (3) After adding the materials in step (2), control the temperature at 105°C, keep stirring for 10 minutes, and control the stirring line speed at 6m / s;

[0041] (4) Put 60 parts of porous ammonium nitrate into the mixer, then add the scrap colloidal emulsion explosive mixture pretreated in step (3), keep the temperature, and stir and mix for 5 minutes according to the process regulations;

[0042] (5) Packaging the product prepared in step (4) with a plastic film to obtain a porous ammonium oil explosive;

[0043] The obtained product used 100g of No. 2 rock emulsion explosive as the primer for detonation ...

Embodiment 3

[0045] The ratio of explosive raw materials is in parts by weight

[0046] (1) Put 4 parts of 10# total loss system oil into the melting tank, and then put in 1 part of surfactant, and control the temperature at 110°C;

[0047] (2) Add 20 parts of scrap colloidal emulsion explosive into the melting tank of step (1), and divide it into small pieces when adding;

[0048] (3) After adding the materials in step (2), control the temperature at 110°C, keep stirring for 8 minutes, and control the stirring line speed at 6m / s;

[0049] (4) Put 75 parts of porous ammonium nitrate into the mixer, then add the pretreated waste colloidal emulsion explosive mixture in step (3), keep the temperature, and stir and mix for 5 minutes according to the process regulations;

[0050] (5) Packaging the product prepared in step (4) with plastic film, namely the porous ammonium oil explosive;

[0051] The obtained product used 100g of No. 2 rock emulsion explosive as the primer for detonation perfor...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention provides a treatment method of a waste colloidal emulsion explosive in a porous ammonium nitrate fuel oil explosive. Namely, the waste colloidal emulsion explosive is pre-treated to be mixed with porous ammonium nitrate or porous ammonium nitrate mixed with a certain amount of oil phase according to a certain ratio; corresponding technical parameters are adjusted according to technical requirements of a product so as to prepare the qualified porous ammonium nitrate fuel oil explosive, wherein a pre-treated waste colloidal emulsion explosive mixed solution accounts for 20.0-40.0% of the total weight of an explosive finished product, and the porous ammonium nitrate or porous ammonium nitrate mixed with the certain amount of oil phase accounts for 60.0-80.0% of the total weight of the explosive finished product. Compared with existing other treatment methods, the treatment method disclosed by the invention is simple in production process technology, and stable and reliable in product quality and has economical and environment-friendly effects; potential quality hazards and potential safety hazards which are generated by online addition of the waste colloidal emulsion explosive, as well as raw material waste and environment pollution which are caused by destroying and treating the waste colloidal emulsion explosive are avoided; the recycling and the reutilization of the waste colloidal emulsion explosive are realized, and the treatment method has more obvious economic benefits and social benefits.

Description

technical field [0001] The invention relates to a treatment method of scrapped industrial explosives, in particular to a treatment method of scrapped colloidal emulsion explosives in porous ammonium oil explosives. Background technique [0002] At present, the processing methods of scrap colloidal emulsion explosives mainly include the following types: [0003] (1) Add processing online. It is mainly aimed at the treatment of latex matrix or finished drug body with good milk quality. For the primary or secondary emulsification medium and low temperature sensitization production line, most of them manually add a small amount and multiple times directly from the feed port of the sensitization machine; for the high temperature sensitization production line, they add a small amount and multiple times from the latex matrix hopper in front of the sensitizing mixer. This method is the most simple and feasible, and most emulsion explosive manufacturers use this method to dispose o...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C06B31/28
Inventor 李玉明张玉健唐帮义蒋莉万炳泉孙玉红艾家圆
Owner SICHUAN YAHUA IND GRP
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products