Embodiment 1
[0009] 30 parts of polyurethane acrylic resin
[0010] Rare Earth Element Activated Alkaline Earth Aluminate 30 parts
[0011] 10 phosphors
[0012] 5 parts of varnish
[0013] 1 part polyethylene wax
[0014] 1 part organic bentonite
[0015] First, 15 parts of urethane acrylic resin, 30 parts of rare earth element activated alkaline earth aluminate, 10 parts of fluorescent powder, 5 parts of tinted ink, 1 part of polyethylene wax, and 1 part of organic bentonite were added to the mixer for 30 minutes at medium speed, and then added 15 parts of urethane acrylic resin are stirred at high speed to make the materials evenly mixed, and finally the finished product is obtained by grinding and dispersing by a three-roller machine.
Embodiment 2
[0017] 55 parts of urethane acrylic resin
[0018] Rare earth element activated alkaline earth aluminate 45 parts
[0019] Phosphor 15 parts
[0020] 8 parts of varnish
[0021] 3 parts polyethylene wax
[0022] 2 parts organic bentonite
[0023] First add 30 parts of urethane acrylic resin, 45 parts of rare earth element activated alkaline earth aluminate, 15 parts of fluorescent powder, 8 parts of tinted ink, 3 parts of polyethylene wax and 2 parts of organobentonite into the mixer for 30 minutes at medium speed, and then add 25 parts of polyurethane acrylic resin are stirred at high speed to make the materials evenly mixed, and finally the finished product is obtained by grinding and dispersing by a three-roller machine.
Embodiment 3
[0025] 80 parts of polyurethane acrylic resin
[0026] Rare earth element activated alkaline earth aluminate 60 parts
[0027] Phosphor 20 copies
[0028] 10 parts of varnish
[0029] Polyethylene wax 5 parts
[0030] 3 parts organic bentonite
[0031] First, 40 parts of polyurethane acrylic resin, 60 parts of rare earth element-activated alkaline earth aluminate, 20 parts of fluorescent powder, 10 parts of tinted ink, 5 parts of polyethylene wax, and 3 parts of organic bentonite were added to the mixer for 30 minutes at medium speed, and then added 40 parts of urethane acrylic resin were stirred at high speed to make the materials evenly mixed, and finally the finished product was obtained by grinding and dispersing by a three-roller machine.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com