Manufacturing method of silk used in machine-washable silk quilt
A production method and technology of silk quilts, which are applied in textiles and papermaking, fiber treatment, animal fibers, etc., to achieve the effects of large ventilation space, improved elasticity, and simplified necessary steps
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0012] The present invention will be described in further detail below in conjunction with the embodiments.
[0013] Example:
[0014] 1) Preparation of solution: chlorotriazine-β-cyclodextrin, mixed with seven-membered melon ring at a weight ratio of 1:5, added water to a concentration of 15 g / L, adjusted the pH to 6.5 with acetic acid, at 25 °C Dissolve with ultrasound for 2 hours at high temperature;
[0015] 2) Immersion grafting: immerse the silk fiber in the solution, the weight ratio of silk fiber:solution is 2:1, the solution temperature is 23°C, and the immersion time is 7 days;
[0016] 3) Rinse the reacted silk fiber and dry it until the water content is ≤12% to obtain the product.
[0017] Example product machine washing test data comparison table
[0018]
[0019] It is found from experiments that the effect of machine washing 20 times after treatment is better than that of untreated machine washing once.