A welding method and Bourdon tube technology, applied in welding equipment, auxiliary welding equipment, welding/cutting auxiliary equipment, etc., can solve the problems of pits in the welding place, easy blockage of through holes, easy corrosion of weld seams, etc., and achieve local The effect of slow flow rate, less weld defects and uniform weld structure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] A Bourdon tube welding device for a pressure gauge, comprising a base 1, a vent pipe 2, a water spray pipe 5, a first groove and a second groove; the first groove and the second groove are arranged on the base 1; the One end of the second groove is vertically connected to the first groove; the air pipe 2 is fixed on the base 1, and one end of the air pipe 2 is arranged in the second groove; the water spray pipe 5 is arranged on the base 1. The cross section of the second groove is a semicircle, the inner diameter of the second groove is equal to 2cm, and the diameter d (inner diameter) of the air pipe 2 is equal to 1cm. The axial centerline of the water spray pipe 5 and the axial centerline of the second groove (the cross section of the second groove is a semicircle, and the centers of all semicircles are connected into a line, which is the second groove The included angle between the axial centerlines) is 135°. The port of the air pipe 2 is provided with a protrusion ...
Embodiment 2
[0043] With embodiment 1, the difference is that the inner diameter of the second groove is equal to 2.4cm, the diameter d (inner diameter) of the air pipe 2 is equal to 0.8cm, and the included angle between the central axis of the air pipe 2 and the central axis of the second groove Be 15 °, the gas that feeds in the step (2) is carbon dioxide. The welded Bourdon tubes had no clogging, and out of 1000 welded products, only 3 were unqualified. And the welding defects are obviously reduced by 70% compared with the welding defects when there is no ventilation. In particular, there is no depression or incomplete penetration of the welds inside the through holes, and the welded Bourdon tubes have not been corroded after one year of use.
Embodiment 3
[0045] With embodiment 1, the difference is that the inner diameter of the second groove is equal to 2.4cm, the diameter d (inner diameter) of the air pipe 2 is equal to 1.2cm, and the included angle between the central axis of the air pipe 2 and the central axis of the second groove is 15°. The welded Bourdon tubes had no clogging, and out of 1000 welded products, only 3 were unqualified. And the welding defects are obviously reduced by 70% compared with the welding defects when there is no ventilation. In particular, there is no depression or incomplete penetration of the welds inside the through holes, and the welded Bourdon tubes have not been corroded after one year of use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com