A kind of anti-adhesive high-strength engineering equipment container processing method
A technology of engineering equipment and processing methods, which is applied in the direction of containers, large containers, packaging, etc., can solve the problems of mechanical properties of transportation equipment and steel structure damage, inconvenient storage, transportation and unloading of materials, and abnormal transfer of muck and soil, etc., to achieve Save sintering time and energy consumption, improve service life, and improve wear resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment 1: a kind of anti-sticking high-strength engineering equipment container processing method, comprises the following steps:
[0016] (1) Surface treatment of the inner surface of the container: First, apply an organic solvent to dissolve the oil on the inner wall of the container and heat it to 400°C, so that all the oil on the inner wall of the container is completely volatilized, and then use sandblasting to mechanically clean the container and make the inner wall rough. Use the nature of organic solvents to dissolve grease to remove oil stains, and use sandblasting to improve the solidification effect of the mixed material on the inner wall of the container after spraying.
[0017] (2) Mixed coating spraying: After mixing high-carbon fiber precursors and paraldehyde according to a certain mass ratio, spray them directly on the inner wall of the container, and then spray polytetrafluoroethylene, paraldehyde and polytetrafluoroethylene The mass ratio is 1:20,...
Embodiment 2
[0020] Embodiment 2: a kind of anti-sticking high-strength engineering equipment container processing method, comprises the following steps:
[0021] (1) The inner surface treatment of the container is the same as in Example 1.
[0022] (2) Mixed coating spraying: After attaching the high-carbon fiber with a network structure on the inner wall of the container, spray paraldehyde first, and then spray polytetrafluoroethylene. The mass ratio of paraldehyde to polytetrafluoroethylene is 1:19, high carbon fiber raw silk can adjust the mixing ratio according to actual needs. The spray coating material must be uniform, and the coating thickness depends on the coating system used. The spraying amount of PTFE is determined according to the coating thickness, and the coating thickness varies from a few microns to 200 microns (0.2 mm). .
[0023] (3) drying, the same as in Example 1.
[0024] (4) Sintering is the same as in Example 1.
[0025] It must be emphasized that the mass rat...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More