Examples
specific Embodiment approach 1
[0019] Embodiment 1: In this embodiment, the medium and low temperature hydraulic oil is composed of 91% HVIS base oil, 3% ethylene-propylene copolymer, 2% polyalphaolefin pour point depressant, 1% 2,6-di-tert-butyl Made of p-cresol antioxidant and 3% sulfur phosphorus type extreme pressure antiwear agent.
[0020] Step 1. Weigh 91% HVIS base oil, 3% ethylene-propylene copolymer, 2% polyalphaolefin pour point depressant, 1% 2,6-di-tert-butyl-p-cresol antioxidant and 3% by weight percentage respectively %Thion type extreme pressure antiwear agent;
[0021] Step 2. Heat up the HVIS base oil weighed in step 1 to 120°C at a rate of 1°C / min, heat-preserve and dehydrate for 30 minutes, and then cool down to 80°C at a rate of 1°C / min;
[0022] Step 3, then add the ethylene-propylene copolymer, polyalphaolefin pour point depressant, 2,6-di-tert-butyl-p-cresol antioxidant and sulfur phosphorus type extreme pressure antiwear agent weighed in step 1;
[0023] Step 4, stirring at 60 r / m...
specific Embodiment approach 2
[0029] Specific embodiment two: In this embodiment, the low-temperature hydraulic oil is composed of 93% HVIS base oil, 1% ethylene-propylene copolymer, 1% polyalphaolefin pour point depressant, 1% thiadiazole derivative and 4% by weight percentage. Made of sulfur phosphorus type extreme pressure antiwear agent.
[0030] Step 1. Weigh 93% of HVIS base oil, 1% of ethylene-propylene copolymer, 1% of polyalphaolefin pour point depressant, 1% of thiadiazole derivatives and 4% of sulfur-phosphorus extreme pressure antiwear agent by weight percentage ;
[0031] Step 2. Heat up the HVIS base oil weighed in step 1 to 120°C at a rate of 1°C / min, heat-preserve and dehydrate for 30 minutes, and then cool down to 80°C at a rate of 1°C / min;
[0032] Step 3, then add the ethylene-propylene copolymer, polyalphaolefin pour point depressant, thiadiazole derivatives and thion-type extreme pressure antiwear agent weighed in step 1;
[0033] Step 4, stirring at 60 r / min for 40 minutes under the...
specific Embodiment approach 3
[0039] Specific embodiment three: In this embodiment, the low-temperature hydraulic oil is composed of 88% HVIS base oil, 4% ethylene-propylene copolymer, 2% polyalphaolefin pour point depressant, 2% thiadiazole derivatives and 4% by weight percentage Made of sulfur phosphorus type extreme pressure antiwear agent.
[0040] Step 1. Weigh 88% of HVIS base oil, 4% of ethylene-propylene copolymer, 2% of polyalphaolefin pour point depressant, 2% of thiadiazole derivatives and 4% of sulfur-phosphorus extreme pressure antiwear agent by weight percentage ;
[0041] Step 2. Heat up the HVIS base oil weighed in step 1 to 120°C at a rate of 1°C / min, heat-preserve and dehydrate for 30 minutes, and then cool down to 80°C at a rate of 1°C / min;
[0042] Step 3, then add the ethylene-propylene copolymer, polyalphaolefin pour point depressant, thiadiazole derivatives and thion-type extreme pressure antiwear agent weighed in step 1;
[0043] Step 4, stirring at 60 r / min for 40 minutes under t...
PUM
Property | Measurement | Unit |
---|---|---|
Solidifying point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com