Technology method of light guide plate or light guide bar for daytime running light
A process method and technology of light guide sheet, applied in the direction of light guide, optics, optical components, etc., can solve the problem of low luminous intensity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] 1. A process method for light guide sheet or light guide strip for daytime running lights, characterized in that the process method consists of the following steps:
[0020] 1) Take two parts of 250g of polymethyl methacrylate, melt them at a melting temperature of 260-300°C, and mold them independently at a mold temperature of 60-80°C to prepare the top sheet of the light guide sheet and the light guide sheet Lower sheet; then apply 1.2g of glue on the upper surface of the lower sheet of the light guide sheet, then evenly spray 5g of calcium halophosphate white phosphor, and finally press the upper cover of the light guide sheet on the upper surface of the lower sheet of the light guide sheet, Under the condition of temperature of 260° C., thermocompression molding is carried out to obtain a light guide sheet.
Embodiment 2
[0022] Take two parts of 250g of polymethyl methacrylate, melt them at a melting temperature of 260-300°C, and mold them independently at a mold temperature of 60-80°C to prepare the upper light guide sheet and the lower light guide sheet Then on the upper surface of the light guide sheet lower sheet, smear 0.8g glue, then evenly spray calcium halophosphate white fluorescent powder 2.5g, finally the upper sheet cover of the light guide sheet is pressed on the upper surface of the light guide sheet lower sheet, Under the condition of temperature of 220° C., thermocompression molding is carried out to obtain a light guide sheet.
Embodiment 3
[0024] Take two parts of 250g of polymethyl methacrylate, melt them at a melting temperature of 260-300°C, and mold them independently at a mold temperature of 60-80°C to prepare the upper light guide sheet and the lower light guide sheet Then on the upper surface of the light guide sheet lower sheet, smear 1g glue, then evenly spray calcium halophosphate white fluorescent powder 2g, finally the upper sheet cover of the light guide sheet is pressed on the upper surface of the light guide sheet lower sheet, at a temperature of Under the condition of 250° C., hot pressing is performed to obtain a light guide sheet.
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More