A kind of additive-free dyeing method of disperse dye
A technology of disperse dyes and dyeing methods, applied in the field of disperse dyes without additives, can solve the problems of increased difficulty and cost of sewage treatment, high treatment technology and cost, large water and energy consumption, etc., to avoid pollution of dyeing wastewater, dyeing The method is convenient and the effect of saving energy
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] At a bath ratio of 1:20, the ratio of water in the container to the dyeing cup is 1:3, and the dosage of disperse dyes (without additives) is: 1% o.w.f. After adding the dye and water to the container, use polytetrafluoroethylene (PTFE) Microporous membrane seal. Then put the sealed container into the dyeing cup, add water and polyester fabric, and carry out high temperature and high pressure dyeing. The dyeing process is as follows: put it in at 40°C, raise it to 120°C at 2°C / min, keep it warm for 1 hour, then lower it to 60°C at 3°C / min, take it out, and wash it with water. After the dye solution in the container is cooled to room temperature, the disperse dyes are recovered by suction filtration and washing.
Embodiment 2
[0024] At a bath ratio of 1:20, the ratio of water in the container to the dyeing cup is 1:5, and the dosage of disperse dyes (without additives) is: 2% o.w.f. After adding the dye and water to the container, use polytetrafluoroethylene (PTFE) Microporous membrane seal. Then put the sealed container into the dyeing cup, add water and polyester fabric, and carry out high temperature and high pressure dyeing. The dyeing process is as follows: put it in at 40°C, raise it to 130°C at 2°C / min, keep it warm for 1 hour, then lower it to 60°C at 3°C / min, take it out, and wash it with water. After the dye solution in the container is cooled to room temperature, the disperse dyes are recovered by suction filtration and washing.
Embodiment 3
[0026] At a bath ratio of 1:30, the ratio of water in the container to the dyeing cup is 1:10, the amount of disperse dye (without additives) is: 3% o.w.f, and the dye and water are added to the container with polytetrafluoroethylene (PTFE) Microporous membrane seal. Then put the sealed container into the dyeing cup, add water and polyester fabric, and carry out high temperature and high pressure dyeing. The dyeing process is as follows: put it in at 40°C, raise it to 140°C at 2°C / min, keep it warm for 1 hour, then lower it to 60°C at 3°C / min, take it out, and wash it with water. After the dye solution in the container is cooled to room temperature, the disperse dyes are recovered by suction filtration and washing.
PUM
Property | Measurement | Unit |
---|---|---|
pore size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com