Deformation oiling agent for copper ammonia fiber high-stretch yarn
A technology of cupro ammonia fiber and high elastic yarn, which is applied in fiber treatment, plant fiber, textiles and papermaking, etc. It can solve the problems of poor effect, achieve uniform elastic force, large elastic shrinkage rate, and expand the application range.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] A cupro ammonia fiber high elastic yarn deformation oil, its components by weight, 100 parts of vaseline, 35 parts of fatty acid trimethylol propyl ester, 20 parts of soybean oil, 14.5 parts of glutathione, palmitate poly 12 parts of oxyethylene ether, 4 parts of dioctyl sebacate, 0.1 part of sodium chloride.
Embodiment 2
[0013] A cupro ammonia fiber high elastic yarn deformation oil, its components by weight, 100 parts of vaseline, 25 parts of fatty acid trimethylol propyl ester, 27 parts of soybean oil, 12 parts of glutathione, palmitate poly 15 parts of oxyethylene ether, 2 parts of dioctyl sebacate, 2 parts of sodium chloride.
Embodiment 3
[0015] A cupro ammonia fiber high elastic yarn deformation oil, its components by weight, 100 parts of vaseline, 40 parts of fatty acid trimethylol propyl ester, 20 parts of soybean oil, 15 parts of glutathione, palmitate poly 10 parts of oxyethylene ether, 8 parts of dioctyl sebacate, and 0.05 parts of sodium chloride.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com