A trademark cloth and green cloth technology, which is applied in the field of easy-to-tear trademark cloth and its preparation, can solve the problems of dislike of consumers and the inconvenience of changing the place of origin, so as to achieve the effect of improving convenience, ensuring yield rate and high quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] Embodiment 1: An easy-to-tear trademark cloth, including a gray cloth layer and a rubber material layer, the gray cloth layer interweaves warp yarns and weft yarns through a loom to form a flat cloth, and the warp yarns and weft yarns are selected from 70 to 100 Dennis acetate yarn, each denier acetate yarn is composed of 12 spun yarns; the warp yarn density is 90 yarns / cm, and the weft yarn density is 80 yarns / cm. The thickness of the gray cloth layer is 90 μm, the thickness of the rubber layer is 15 μm; the thickness of the trademark cloth is 105 μm, and the weight of the trademark cloth is 80 g / m 2 . The rubber layer contains 60wt% thermosetting polymer, 15wt% diluent, 15wt% filler powder and 10wt% additive.
[0014] The preparation method of the above-mentioned easy-to-tear label cloth comprises the following steps:
[0015] (1) Gray cloth layer weaving: the warp and weft yarns are interwoven by the loom to form a flat fabric. The warp and weft yarns are selected ...
Embodiment 2
[0018] Embodiment 2: An easy-to-tear trademark cloth, including a gray cloth layer and a rubber layer, the gray cloth layer interweaves warp yarns and weft yarns through a loom to form a flat cloth, and the warp yarns and weft yarns are selected from 70 to 100 Dennis acetate yarn, each Dennis acetate yarn is composed of 20 spun yarns; the warp yarn density is 100 yarns / cm, and the weft yarn density is 70 yarns / cm. The thickness of the gray cloth layer is 100 μm, the thickness of the rubber layer is 20 μm; the thickness of the trademark cloth is 120 μm, and the weight of the trademark cloth is 95 g / m 2 . The rubber layer contains 60 wt% of thermosetting high molecular polymer, 20 wt% of diluent, 10 wt% of filler powder and 10 wt% of additives.
[0019] The preparation method of the above-mentioned easy-to-tear label cloth comprises the following steps:
[0020] (1) Gray cloth layer weaving: the warp and weft yarns are interwoven by the loom to form a flat fabric. The warp and...
Embodiment 3
[0023] Embodiment 3: An easy-to-tear trademark cloth, including a gray cloth layer and a rubber layer, the gray cloth layer is interwoven with warp yarns and weft yarns by a loom to form a flat cloth, and the warp yarns and weft yarns are selected from 70 to 100 Dennis acetate yarn, each denier acetate yarn is composed of 36 spun yarns; the warp yarn density is 110 yarns / cm, and the weft yarn density is 80 yarns / cm. The thickness of the gray cloth layer is 110 μm, the thickness of the rubber layer is 10 μm; the thickness of the trademark cloth is 120 μm, and the weight of the trademark cloth is 90 g / m 2 . The rubber layer contains 75 wt% of thermosetting high molecular polymer, 15 wt% of diluent, 5 wt% of filler powder and 5 wt% of additives.
[0024] The preparation method of the above-mentioned easy-to-tear label cloth comprises the following steps:
[0025] (1) Gray cloth layer weaving: the warp and weft yarns are interwoven by the loom to form a flat fabric. The warp and...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com